Transparent semiconducting SrTiO(3) crystal fabricated by heating treatment with gaseous ammonia and CeO(2) powder
A transparent semiconducting SrTiO(3) single crystal with a resistivity of the order of 10(3) Ω·cm was fabricated by heating a SrTiO(3) single crystal with gaseous ammonia and CeO(2) powder. Conductive atomic force microscope (C-AFM) measurement revealed that micro-sized voids were formed and the hi...
Autores principales: | Morimoto, Yuka, Nishiyama, Junji, Takeda, Hiroaki, Tsurumi, Takaaki, Hoshina, Takuya |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group UK
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5864887/ https://www.ncbi.nlm.nih.gov/pubmed/29568047 http://dx.doi.org/10.1038/s41598-018-23019-9 |
Ejemplares similares
-
Electronic properties and surface reactivity of SrO-terminated SrTiO(3) and SrO-terminated iron-doped SrTiO(3)
por: Staykov, Aleksandar, et al.
Publicado: (2018) -
Ce=O Terminated CeO(2)
por: Grinter, David C., et al.
Publicado: (2021) -
Microscopic characterization of Fe nanoparticles formed on SrTiO(3)(001) and SrTiO(3)(110) surfaces
por: Tanaka, Miyoko
Publicado: (2016) -
Structural properties of ultrathin SrO film deposited on SrTiO(3)
por: Gagnidze, Tornike, et al.
Publicado: (2019) -
Unconventional Transport through Graphene on SrTiO(3): A Plausible Effect of SrTiO(3) Phase-Transitions
por: Saha, Surajit, et al.
Publicado: (2014)