Tensile behavior of Cu-coated Pd(40)Cu(30)Ni(10)P(20) metallic glassy wire
Catastrophic brittle fracture of monolithic metallic glass (MG) hinders engineering application of MGs. Although many techniques has been tried to enhance tensile ductility of metallic glasses, the enhancement is quite limited. Here, we show the effect of electrodeposited Cu coating on tensile plast...
Autores principales: | Hussain, I., Jiang, Y. Y., Jia, Y. D., Wang, G., Zhai, Q. J., Chan, K. C., Yi, J. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group UK
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5884840/ https://www.ncbi.nlm.nih.gov/pubmed/29618755 http://dx.doi.org/10.1038/s41598-018-23956-5 |
Ejemplares similares
-
Machinability and Surface Generation of Pd(40)Ni(10)Cu(30)P(20) Bulk Metallic Glass in Single-Point Diamond Turning
por: Xiong, Jie, et al.
Publicado: (2019) -
Comparative Reliability Studies and Analysis of Au, Pd-Coated Cu and Pd-Doped Cu Wire in Microelectronics Packaging
por: Chong Leong, Gan, et al.
Publicado: (2013) -
Correction: Comparative Reliability Studies and Analysis of Au, Pd-Coated Cu and Pd-Doped Cu Wire in Microelectronics Packaging
por: Chong Leong, Gan, et al.
Publicado: (2014) -
Synthesis, and characterization of metallic glassy Cu–Zr–Ni powders decorated with big cube Zr(2)Ni nanoparticles for potential antibiofilm coating applications
por: Aldhameer, Ahmad, et al.
Publicado: (2022) -
Mechanical Alloying Integrated with Cold Spray Coating for Fabrication Cu(50)(Ti(50−x)Ni(x)), x; 10, 20, 30, and 40 at.% Antibiofilm Metallic Glass Coated/SUS304 Sheets
por: Aldhameer, Ahmad, et al.
Publicado: (2022)