Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin
Background. This study was undertaken to evaluate the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin after surface preparation with Nd:YAG and Er,Cr:YSGG lasers. Methods. A total of 102 lithium disilicate glass ceramic samples (IPS e.max Press), measurin...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Tabriz University of Medical Sciences
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5928469/ https://www.ncbi.nlm.nih.gov/pubmed/29732016 http://dx.doi.org/10.15171/joddd.2018.003 |
_version_ | 1783319248659021824 |
---|---|
author | Ebrahimi Chaharom, Mohammad Esmaeel Pournaghi Azar, Fatemeh Mohammadi, Narmin Nasiri, Rezvan |
author_facet | Ebrahimi Chaharom, Mohammad Esmaeel Pournaghi Azar, Fatemeh Mohammadi, Narmin Nasiri, Rezvan |
author_sort | Ebrahimi Chaharom, Mohammad Esmaeel |
collection | PubMed |
description | Background. This study was undertaken to evaluate the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin after surface preparation with Nd:YAG and Er,Cr:YSGG lasers. Methods. A total of 102 lithium disilicate glass ceramic samples (IPS e.max Press), measuring 5 mm in diameter and 4 mm in thickness, were randomly assigned to 6 groups (n=17): group 1, no surface preparation (control); group 2, acid etching with 9.5% hydrofluoric acid (HF); group 3, surface preparation with 4.5-W Nd:YAG laser; group 4, surface preparation with 6-W Nd:YAG laser; group 5, surface preparation with 1.5-W Er,Cr:YSGG laser; and group 6, surface preparation with 6-W Er,Cr:YSGG laser. After preparation of surfaces and application of silane, all the samples were repaired with the use of a silorane-based composite resin, followed by storage in distilled water at a temperature of 37°C for 24 hours and thermocycling. Finally, the samples were subjected to a shearing bond strength test; the fracture modes were determined under a stereomi-croscope. Results. There were significant differences between the HF group and the other groups (P=0.000). Two-by-two comparisons of the other groups revealed no significant differences (P>0.05). Conclusion. Use of HF proved the most effective surface preparation technique to increase the repair bond strength between lithium disilicate glass ceramic and silorane-based composite resin; compared to the control group. |
format | Online Article Text |
id | pubmed-5928469 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2018 |
publisher | Tabriz University of Medical Sciences |
record_format | MEDLINE/PubMed |
spelling | pubmed-59284692018-05-04 Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin Ebrahimi Chaharom, Mohammad Esmaeel Pournaghi Azar, Fatemeh Mohammadi, Narmin Nasiri, Rezvan J Dent Res Dent Clin Dent Prospects Original Article Background. This study was undertaken to evaluate the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin after surface preparation with Nd:YAG and Er,Cr:YSGG lasers. Methods. A total of 102 lithium disilicate glass ceramic samples (IPS e.max Press), measuring 5 mm in diameter and 4 mm in thickness, were randomly assigned to 6 groups (n=17): group 1, no surface preparation (control); group 2, acid etching with 9.5% hydrofluoric acid (HF); group 3, surface preparation with 4.5-W Nd:YAG laser; group 4, surface preparation with 6-W Nd:YAG laser; group 5, surface preparation with 1.5-W Er,Cr:YSGG laser; and group 6, surface preparation with 6-W Er,Cr:YSGG laser. After preparation of surfaces and application of silane, all the samples were repaired with the use of a silorane-based composite resin, followed by storage in distilled water at a temperature of 37°C for 24 hours and thermocycling. Finally, the samples were subjected to a shearing bond strength test; the fracture modes were determined under a stereomi-croscope. Results. There were significant differences between the HF group and the other groups (P=0.000). Two-by-two comparisons of the other groups revealed no significant differences (P>0.05). Conclusion. Use of HF proved the most effective surface preparation technique to increase the repair bond strength between lithium disilicate glass ceramic and silorane-based composite resin; compared to the control group. Tabriz University of Medical Sciences 2018 2018-03-14 /pmc/articles/PMC5928469/ /pubmed/29732016 http://dx.doi.org/10.15171/joddd.2018.003 Text en © 2018 Ebrahimi Chaharom et al. http://creativecommons.org/licenses/by/4.0/ This is an Open Access article published and distributed by Tabriz University of Medical Sciences under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by/4.0), which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited. |
spellingShingle | Original Article Ebrahimi Chaharom, Mohammad Esmaeel Pournaghi Azar, Fatemeh Mohammadi, Narmin Nasiri, Rezvan Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
title | Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
title_full | Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
title_fullStr | Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
title_full_unstemmed | Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
title_short | Effect of surface preparation with Nd:YAG and Er,Cr:YSGG lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
title_sort | effect of surface preparation with nd:yag and er,cr:ysgg lasers on the repair bond strength of lithium disilicate glass ceramic to a silorane-based composite resin |
topic | Original Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5928469/ https://www.ncbi.nlm.nih.gov/pubmed/29732016 http://dx.doi.org/10.15171/joddd.2018.003 |
work_keys_str_mv | AT ebrahimichaharommohammadesmaeel effectofsurfacepreparationwithndyagandercrysgglasersontherepairbondstrengthoflithiumdisilicateglassceramictoasiloranebasedcompositeresin AT pournaghiazarfatemeh effectofsurfacepreparationwithndyagandercrysgglasersontherepairbondstrengthoflithiumdisilicateglassceramictoasiloranebasedcompositeresin AT mohammadinarmin effectofsurfacepreparationwithndyagandercrysgglasersontherepairbondstrengthoflithiumdisilicateglassceramictoasiloranebasedcompositeresin AT nasirirezvan effectofsurfacepreparationwithndyagandercrysgglasersontherepairbondstrengthoflithiumdisilicateglassceramictoasiloranebasedcompositeresin |