Tribological Behavior and the Mild–Severe Wear Transition of Mg97Zn1Y2 Alloy with a LPSO Structure Phase
Dry friction and wear tests were performed on as-cast Mg97Zn1Y2 alloy using a pin-on-disc configuration. Coefficients of friction and wear rates were measured as a function of applied load at sliding speeds of 0.2, 0.8 and 3.0 m/s. The wear mechanisms were identified in the mild and severe wear regi...
Autores principales: | Sun, Wei, Xuan, Xihua, Li, Liang, An, Jian |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5951351/ https://www.ncbi.nlm.nih.gov/pubmed/29584692 http://dx.doi.org/10.3390/ma11040505 |
Ejemplares similares
-
Dry Sliding Wear Behavior and Mild–Severe Wear Transition of Mg97Zn1Y2 Alloy at Elevated Temperatures
por: Li, Liang, et al.
Publicado: (2018) -
Role of LPSO Phase in Crack Propagation Behavior of an As-Cast Mg-Y-Zn Alloy Subjected to Dynamic Loadings
por: Shi, Xuezhi, et al.
Publicado: (2019) -
Comparison of Thermal Deformation Behavior and Characteristics of Mg-Gd-Y-Zn Alloys with and without Bulk LPSO Phase
por: Chen, Dongjie, et al.
Publicado: (2023) -
The effect of silica NPs incorporation on protective properties of oxide layers formed by PEO on Mg(97)Y(2)Zn(1) alloy with LPSO-phase
por: Krishtal, M.M., et al.
Publicado: (2023) -
Kink-band formation in the directionally-solidified Mg/LPSO two-phase alloys
por: Tokunaga, Toko, et al.
Publicado: (2022)