Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)

This study was conducted with the aim of achieving the simultaneous screening of various additives in polymer materials by utilizing a solvent-free pyrolyzer/thermal desorption gas chromatography mass spectrometry (Py/TD-GC–MS) method. As a first step to achieve this goal, simultaneous screening has...

Descripción completa

Detalles Bibliográficos
Autores principales: Yanagisawa, Hiroyuki, Kudo, Yukihiko, Nakagawa, Katsuhiro, Miyagawa, Haruhiko, Maruyama, Fumitaka, Fujimaki, Shigehiko
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6017896/
https://www.ncbi.nlm.nih.gov/pubmed/29565319
http://dx.doi.org/10.3390/molecules23040728
_version_ 1783334850939322368
author Yanagisawa, Hiroyuki
Kudo, Yukihiko
Nakagawa, Katsuhiro
Miyagawa, Haruhiko
Maruyama, Fumitaka
Fujimaki, Shigehiko
author_facet Yanagisawa, Hiroyuki
Kudo, Yukihiko
Nakagawa, Katsuhiro
Miyagawa, Haruhiko
Maruyama, Fumitaka
Fujimaki, Shigehiko
author_sort Yanagisawa, Hiroyuki
collection PubMed
description This study was conducted with the aim of achieving the simultaneous screening of various additives in polymer materials by utilizing a solvent-free pyrolyzer/thermal desorption gas chromatography mass spectrometry (Py/TD-GC–MS) method. As a first step to achieve this goal, simultaneous screening has been examined by selecting major substances representing plasticizers and flame retardants, such as short chain chlorinated paraffins (SCCPs), decabromodiphenyl ether (DecaBDE), hexabromocyclododecane (HBCDD), and di(2-ethylhexyl) phthalate (DEHP). A quantitative MS analysis was performed to check for the peak areas and sensitivities. Since Py/TD-GC–MS is fraught with the risk of thermal degradation of the sample, temperatures during the analytical process were finely tuned for securing reliable results. The instrumental sensitivity was confirmed by the S/N ratio on each component. The detection limits of all components were less than 50 mg/kg, which are sufficiently lower than the regulatory criteria. With regard to reproducibility, a relative standard deviation (RSD) of about 5% was confirmed by employing a spike recovery test on a polystyrene polymer solution containing mixed standard solution (ca. 1000 mg/kg). In conclusion, the results obtained in this study indicate that Py/TD-GC–MS is applicable for the screening of major flame retardants and plasticizers in real samples with sufficient reproducibility at regulatory levels.
format Online
Article
Text
id pubmed-6017896
institution National Center for Biotechnology Information
language English
publishDate 2018
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-60178962018-11-13 Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS) Yanagisawa, Hiroyuki Kudo, Yukihiko Nakagawa, Katsuhiro Miyagawa, Haruhiko Maruyama, Fumitaka Fujimaki, Shigehiko Molecules Article This study was conducted with the aim of achieving the simultaneous screening of various additives in polymer materials by utilizing a solvent-free pyrolyzer/thermal desorption gas chromatography mass spectrometry (Py/TD-GC–MS) method. As a first step to achieve this goal, simultaneous screening has been examined by selecting major substances representing plasticizers and flame retardants, such as short chain chlorinated paraffins (SCCPs), decabromodiphenyl ether (DecaBDE), hexabromocyclododecane (HBCDD), and di(2-ethylhexyl) phthalate (DEHP). A quantitative MS analysis was performed to check for the peak areas and sensitivities. Since Py/TD-GC–MS is fraught with the risk of thermal degradation of the sample, temperatures during the analytical process were finely tuned for securing reliable results. The instrumental sensitivity was confirmed by the S/N ratio on each component. The detection limits of all components were less than 50 mg/kg, which are sufficiently lower than the regulatory criteria. With regard to reproducibility, a relative standard deviation (RSD) of about 5% was confirmed by employing a spike recovery test on a polystyrene polymer solution containing mixed standard solution (ca. 1000 mg/kg). In conclusion, the results obtained in this study indicate that Py/TD-GC–MS is applicable for the screening of major flame retardants and plasticizers in real samples with sufficient reproducibility at regulatory levels. MDPI 2018-03-22 /pmc/articles/PMC6017896/ /pubmed/29565319 http://dx.doi.org/10.3390/molecules23040728 Text en © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Yanagisawa, Hiroyuki
Kudo, Yukihiko
Nakagawa, Katsuhiro
Miyagawa, Haruhiko
Maruyama, Fumitaka
Fujimaki, Shigehiko
Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)
title Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)
title_full Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)
title_fullStr Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)
title_full_unstemmed Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)
title_short Simultaneous Screening of Major Flame Retardants and Plasticizers in Polymer Materials Using Pyrolyzer/Thermal Desorption Gas Chromatography Mass Spectrometry (Py/TD–GC–MS)
title_sort simultaneous screening of major flame retardants and plasticizers in polymer materials using pyrolyzer/thermal desorption gas chromatography mass spectrometry (py/td–gc–ms)
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6017896/
https://www.ncbi.nlm.nih.gov/pubmed/29565319
http://dx.doi.org/10.3390/molecules23040728
work_keys_str_mv AT yanagisawahiroyuki simultaneousscreeningofmajorflameretardantsandplasticizersinpolymermaterialsusingpyrolyzerthermaldesorptiongaschromatographymassspectrometrypytdgcms
AT kudoyukihiko simultaneousscreeningofmajorflameretardantsandplasticizersinpolymermaterialsusingpyrolyzerthermaldesorptiongaschromatographymassspectrometrypytdgcms
AT nakagawakatsuhiro simultaneousscreeningofmajorflameretardantsandplasticizersinpolymermaterialsusingpyrolyzerthermaldesorptiongaschromatographymassspectrometrypytdgcms
AT miyagawaharuhiko simultaneousscreeningofmajorflameretardantsandplasticizersinpolymermaterialsusingpyrolyzerthermaldesorptiongaschromatographymassspectrometrypytdgcms
AT maruyamafumitaka simultaneousscreeningofmajorflameretardantsandplasticizersinpolymermaterialsusingpyrolyzerthermaldesorptiongaschromatographymassspectrometrypytdgcms
AT fujimakishigehiko simultaneousscreeningofmajorflameretardantsandplasticizersinpolymermaterialsusingpyrolyzerthermaldesorptiongaschromatographymassspectrometrypytdgcms