Mechanical Milling-Assisted Spark Plasma Sintering of Fine-Grained W-Ni-Mn Alloy
Fine-grained W-6Ni-4Mn alloys were fabricated by spark plasma sintering (SPS) using mechanical milling W, Ni and Mn composite powders. The relative density of W-6Ni-4Mn alloy increases from 71.56% to 99.60% when it is sintered at a low temperature range of 1000–1200 °C for 3 min. The spark plasma si...
Autores principales: | Pan, Yanlin, Xiang, Daoping, Wang, Ning, Li, Hui, Fan, Zhishuai |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6117905/ https://www.ncbi.nlm.nih.gov/pubmed/30065176 http://dx.doi.org/10.3390/ma11081323 |
Ejemplares similares
-
The Influence of Milling and Spark Plasma Sintering on the Microstructure and Properties of the Al7075 Alloy
por: Molnárová, Orsolya, et al.
Publicado: (2018) -
Data on the impact of increasing the W amount on the mass density and compressive properties of Ni–W alloys processed by spark plasma sintering
por: Sadat, T., et al.
Publicado: (2016) -
High-Strength Ultra-Fine-Grained Hypereutectic Al-Si-Fe-X (X = Cr, Mn) Alloys Prepared by Short-Term Mechanical Alloying and Spark Plasma Sintering
por: Průša, Filip, et al.
Publicado: (2016) -
Effect of Short Attritor-Milling of Magnesium Alloy Powder Prior to Spark Plasma Sintering
por: Minárik, Peter, et al.
Publicado: (2020) -
Ultrafine-Grained Zn–Mg–Sr Alloy Synthesized by Mechanical Alloying and Spark Plasma Sintering
por: Nečas, David, et al.
Publicado: (2022)