Aging Response and Precipitation Behavior after 5% Pre-Deformation of an Al-Mg-Si-Cu Alloy

In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then pre-deformed for 5% before aging. The peak hardness and yield strength of the pre-deformed sample with subsequent artificial aging were similar to that of a T6 condition sample. It was also found that...