Evaluation of some mechanical properties of a new silicone elastomer for maxillofacial prostheses after addition of intrinsic pigments
OBJECTIVE: The approximate life span of a silicone maxillofacial prosthesis is as short as 1.5–2 years of clinical service, then a new prosthesis should be fabricated. The most common reason for re-making the prosthesis is silicone mechanical properties degradation. The aim of this study was to asse...
Autores principales: | Abdullah, Hussein A., Abdul-Ameer, Faiza M. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Elsevier
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6128324/ https://www.ncbi.nlm.nih.gov/pubmed/30202170 http://dx.doi.org/10.1016/j.sdentj.2018.05.006 |
Ejemplares similares
-
Effect of nano-titanium oxide addition on some mechanical properties of silicone elastomers for maxillofacial prostheses
por: Shakir, Dhuha A., et al.
Publicado: (2018) -
Impact of a mixture of nanofiller and intrinsic pigment on tear strength and hardness of two types of maxillofacial silicone elastomers
por: Abdul-Ameer, Faiza M.
Publicado: (2020) -
Effect of Surface Treated Silicon Dioxide Nanoparticles on Some Mechanical Properties of Maxillofacial Silicone Elastomer
por: Zayed, Sara M., et al.
Publicado: (2014) -
Corrigendum to “Evaluation of Some Mechanical Properties of a Maxillofacial Silicon Elastomer Reinforced with Polyester Powder”
por: Haider, Yagthan Mohammed, et al.
Publicado: (2020) -
Mechanical and Morphological Effect of Plant Based Antimicrobial Solutions on Maxillofacial Silicone Elastomer
por: Tetteh, Sophia, et al.
Publicado: (2018)