Cargando…

A Comparative Study on the Addition Methods of TiO(2) Sintering Aid to the Properties of Porous Alumina Membrane Support

TiO(2) is usually used as a sintering aid to lower the sintering temperature of porous alumina membrane support. Two ways of the addition of TiO(2) are chosen: in-situ precipitation and in-situ hydrolysis. The results show that the distribution status of TiO(2) has an important effect on the propert...

Descripción completa

Detalles Bibliográficos
Autores principales: Yang, Yulong, Chang, Qibing, Hu, Zhiwen, Zhang, Xiaozhen
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6161020/
https://www.ncbi.nlm.nih.gov/pubmed/30044442
http://dx.doi.org/10.3390/membranes8030049
Descripción
Sumario:TiO(2) is usually used as a sintering aid to lower the sintering temperature of porous alumina membrane support. Two ways of the addition of TiO(2) are chosen: in-situ precipitation and in-situ hydrolysis. The results show that the distribution status of TiO(2) has an important effect on the property of porous alumina membrane support. In in-situ hydrolysis method, the nano-meter scale TiO(2) distributes evenly on the alumina particles’ surface. The bending strength of the support increases sharply and the pore size distribution changes more sharply along with the content of TiO(2) which slightly increases from 0.3 wt.% to 0.4 wt.%. The distribution of the nano-meter scale TiO(2) is not so even added by in-situ precipitation method. Neither the bending strength nor the pore size distribution of the support is worse than that of the support added by in-situ hydrolysis even if the content of TiO(2) is high to 2 wt.%. The permeating flux has a similar tendency. Consequently, the porous alumina membrane support has the porosity of 30.01% and the bending strength of 77.33 MPa after sintering at 1650 °C for 2 h with the optimized TiO(2) content of 0.4 wt.% added by the in-situ hydrolysis method.