Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing

PURPOSE: The purpose of this study was to evaluate the marginal discrepancy of heat-pressed ceramic veneers manufactured using a CAD/CAM system. MATERIALS AND METHODS: The ceramic veneers for the abutment of a maxillary left central incisor were designed using a CAD/CAM software program. Ten veneers...

Descripción completa

Detalles Bibliográficos
Autores principales: Kang, Seen-Young, Lee, Ha-Na, Kim, Ji-Hwan, Kim, Woong-Chul
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Korean Academy of Prosthodontics 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6202431/
https://www.ncbi.nlm.nih.gov/pubmed/30370025
http://dx.doi.org/10.4047/jap.2018.10.5.347
_version_ 1783365679615836160
author Kang, Seen-Young
Lee, Ha-Na
Kim, Ji-Hwan
Kim, Woong-Chul
author_facet Kang, Seen-Young
Lee, Ha-Na
Kim, Ji-Hwan
Kim, Woong-Chul
author_sort Kang, Seen-Young
collection PubMed
description PURPOSE: The purpose of this study was to evaluate the marginal discrepancy of heat-pressed ceramic veneers manufactured using a CAD/CAM system. MATERIALS AND METHODS: The ceramic veneers for the abutment of a maxillary left central incisor were designed using a CAD/CAM software program. Ten veneers using a micro-stereolithography apparatus (AM group), ten veneers using a five-axis milling machine (SM group), and ten veneers using a traditional free-hand wax technique (TW group) were prepared according to the respective manufacturing method. The ceramic veneers were also fabricated using a heat-press technique, and a silicone replica was used to measure their marginal discrepancy. The marginal discrepancies were measured using a digital microscope (×160 magnification). The data were analyzed using a nonparametric Kruskal-Wallis H test. Finally, post-hoc comparisons were conducted using Bonferroni-corrected Mann-Whitney U tests (α=.05). RESULTS: The mean±SD of the total marginal discrepancy was 99.68±28.01 µm for the AM group, 76.60±28.76 µm for the SM group, and 83.08±39.74 µm for the TW group. There were significant differences in the total marginal discrepancies of the ceramic veneers (P<.05). CONCLUSION: The SM group showed a better fit than the AM and TW groups. However, all values were within the clinical tolerance. Therefore, CAD/CAM manufacturing methods can replace the traditional free-hand wax technique.
format Online
Article
Text
id pubmed-6202431
institution National Center for Biotechnology Information
language English
publishDate 2018
publisher The Korean Academy of Prosthodontics
record_format MEDLINE/PubMed
spelling pubmed-62024312018-10-26 Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing Kang, Seen-Young Lee, Ha-Na Kim, Ji-Hwan Kim, Woong-Chul J Adv Prosthodont Original Article PURPOSE: The purpose of this study was to evaluate the marginal discrepancy of heat-pressed ceramic veneers manufactured using a CAD/CAM system. MATERIALS AND METHODS: The ceramic veneers for the abutment of a maxillary left central incisor were designed using a CAD/CAM software program. Ten veneers using a micro-stereolithography apparatus (AM group), ten veneers using a five-axis milling machine (SM group), and ten veneers using a traditional free-hand wax technique (TW group) were prepared according to the respective manufacturing method. The ceramic veneers were also fabricated using a heat-press technique, and a silicone replica was used to measure their marginal discrepancy. The marginal discrepancies were measured using a digital microscope (×160 magnification). The data were analyzed using a nonparametric Kruskal-Wallis H test. Finally, post-hoc comparisons were conducted using Bonferroni-corrected Mann-Whitney U tests (α=.05). RESULTS: The mean±SD of the total marginal discrepancy was 99.68±28.01 µm for the AM group, 76.60±28.76 µm for the SM group, and 83.08±39.74 µm for the TW group. There were significant differences in the total marginal discrepancies of the ceramic veneers (P<.05). CONCLUSION: The SM group showed a better fit than the AM and TW groups. However, all values were within the clinical tolerance. Therefore, CAD/CAM manufacturing methods can replace the traditional free-hand wax technique. The Korean Academy of Prosthodontics 2018-10 2018-10-22 /pmc/articles/PMC6202431/ /pubmed/30370025 http://dx.doi.org/10.4047/jap.2018.10.5.347 Text en © 2018 The Korean Academy of Prosthodontics http://creativecommons.org/licenses/by-nc/3.0/ This is an Open Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
spellingShingle Original Article
Kang, Seen-Young
Lee, Ha-Na
Kim, Ji-Hwan
Kim, Woong-Chul
Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing
title Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing
title_full Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing
title_fullStr Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing
title_full_unstemmed Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing
title_short Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing
title_sort evaluation of marginal discrepancy of pressable ceramic veneer fabricated using cad/cam system: additive and subtractive manufacturing
topic Original Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6202431/
https://www.ncbi.nlm.nih.gov/pubmed/30370025
http://dx.doi.org/10.4047/jap.2018.10.5.347
work_keys_str_mv AT kangseenyoung evaluationofmarginaldiscrepancyofpressableceramicveneerfabricatedusingcadcamsystemadditiveandsubtractivemanufacturing
AT leehana evaluationofmarginaldiscrepancyofpressableceramicveneerfabricatedusingcadcamsystemadditiveandsubtractivemanufacturing
AT kimjihwan evaluationofmarginaldiscrepancyofpressableceramicveneerfabricatedusingcadcamsystemadditiveandsubtractivemanufacturing
AT kimwoongchul evaluationofmarginaldiscrepancyofpressableceramicveneerfabricatedusingcadcamsystemadditiveandsubtractivemanufacturing