Cargando…
Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder
Si(3)N(4) ceramics and 304 stainless steel were brazed by Ti40Zr25B0.2Cu amorphous solder, and the interfacial microstructure of brazed joint Si(3)N(4) ceramics/Ti40Zr25B0.2Cu/Cu/Ti40Zr25B0.2Cu/304 stainless steel was analyzed. The mechanical properties of the brazed joint were overtly affected by t...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6265858/ https://www.ncbi.nlm.nih.gov/pubmed/30423903 http://dx.doi.org/10.3390/ma11112226 |
_version_ | 1783375709679386624 |
---|---|
author | Xu, Xiangping Wang, Yi Zou, Jiasheng Xia, Chunzhi |
author_facet | Xu, Xiangping Wang, Yi Zou, Jiasheng Xia, Chunzhi |
author_sort | Xu, Xiangping |
collection | PubMed |
description | Si(3)N(4) ceramics and 304 stainless steel were brazed by Ti40Zr25B0.2Cu amorphous solder, and the interfacial microstructure of brazed joint Si(3)N(4) ceramics/Ti40Zr25B0.2Cu/Cu/Ti40Zr25B0.2Cu/304 stainless steel was analyzed. The mechanical properties of the brazed joint were overtly affected by the brazing temperature and Cu foil thickness. The results revealed that the interface structure of the brazed joint might be 304 stainless steel/FeTi/Cu-Zr+Cu-Ti+Fe-Ti/Cu(s,s)/Cu-Zr+Cu-Ti+Fe-Ti/Ti-Si+Zr-Si/TiN/Si(3)N(4) ceramics. The four-point bending strength of the brazed joint decreased sharply as the brazing temperature increased and reached a maximum of 76 MPa at 1223 K. Furthermore, as the Cu foil thickness was increased from 500 μm to 1000 μm, the joint strength rose to 90 MPa at 1223 K. |
format | Online Article Text |
id | pubmed-6265858 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2018 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-62658582018-12-17 Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder Xu, Xiangping Wang, Yi Zou, Jiasheng Xia, Chunzhi Materials (Basel) Article Si(3)N(4) ceramics and 304 stainless steel were brazed by Ti40Zr25B0.2Cu amorphous solder, and the interfacial microstructure of brazed joint Si(3)N(4) ceramics/Ti40Zr25B0.2Cu/Cu/Ti40Zr25B0.2Cu/304 stainless steel was analyzed. The mechanical properties of the brazed joint were overtly affected by the brazing temperature and Cu foil thickness. The results revealed that the interface structure of the brazed joint might be 304 stainless steel/FeTi/Cu-Zr+Cu-Ti+Fe-Ti/Cu(s,s)/Cu-Zr+Cu-Ti+Fe-Ti/Ti-Si+Zr-Si/TiN/Si(3)N(4) ceramics. The four-point bending strength of the brazed joint decreased sharply as the brazing temperature increased and reached a maximum of 76 MPa at 1223 K. Furthermore, as the Cu foil thickness was increased from 500 μm to 1000 μm, the joint strength rose to 90 MPa at 1223 K. MDPI 2018-11-09 /pmc/articles/PMC6265858/ /pubmed/30423903 http://dx.doi.org/10.3390/ma11112226 Text en © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Xu, Xiangping Wang, Yi Zou, Jiasheng Xia, Chunzhi Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder |
title | Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder |
title_full | Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder |
title_fullStr | Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder |
title_full_unstemmed | Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder |
title_short | Interfacial Microstructure and Properties of Si(3)N(4) Ceramics/Cu/304 Stainless Steel Brazed by Ti40Zr25B0.2Cu Amorphous Solder |
title_sort | interfacial microstructure and properties of si(3)n(4) ceramics/cu/304 stainless steel brazed by ti40zr25b0.2cu amorphous solder |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6265858/ https://www.ncbi.nlm.nih.gov/pubmed/30423903 http://dx.doi.org/10.3390/ma11112226 |
work_keys_str_mv | AT xuxiangping interfacialmicrostructureandpropertiesofsi3n4ceramicscu304stainlesssteelbrazedbyti40zr25b02cuamorphoussolder AT wangyi interfacialmicrostructureandpropertiesofsi3n4ceramicscu304stainlesssteelbrazedbyti40zr25b02cuamorphoussolder AT zoujiasheng interfacialmicrostructureandpropertiesofsi3n4ceramicscu304stainlesssteelbrazedbyti40zr25b02cuamorphoussolder AT xiachunzhi interfacialmicrostructureandpropertiesofsi3n4ceramicscu304stainlesssteelbrazedbyti40zr25b02cuamorphoussolder |