Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma
(1) Background. Titanium is characterized by its biocompatibility, resistance to maximum stress, and fatigue and non-toxicity. The composition, surface structure, and roughness of titanium have a key and direct influence on the osseointegration processes when it is used in the form of dental implant...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6306932/ https://www.ncbi.nlm.nih.gov/pubmed/30544972 http://dx.doi.org/10.3390/jfb9040071 |
_version_ | 1783382888312471552 |
---|---|
author | Rizo-Gorrita, María Luna-Oliva, Irene Serrera-Figallo, María-Angeles Torres-Lagares, Daniel |
author_facet | Rizo-Gorrita, María Luna-Oliva, Irene Serrera-Figallo, María-Angeles Torres-Lagares, Daniel |
author_sort | Rizo-Gorrita, María |
collection | PubMed |
description | (1) Background. Titanium is characterized by its biocompatibility, resistance to maximum stress, and fatigue and non-toxicity. The composition, surface structure, and roughness of titanium have a key and direct influence on the osseointegration processes when it is used in the form of dental implants. The objective of the present study is to characterize, at chemical, superficial, and biological levels, the result of the application of the sandblasted with large-grit and acid-etched (SLA) treatment consisting of coarse-grained and double-passivated acid blasting with subsequent decontamination with argon plasma on the surface of titanium implants type IV. (2) Methods. Four Oxtein(®) dental implants (Zaragoza, Spain) were investigated with the following coding: Code L63713T (titanium grade IV, 3.75 mm in diameter, and 13 mm in length). The surface of the implants was SLA type obtained from coarse-grained, double passivated acid, and decontaminated with argon plasma. The samples were in their sealed packages and were opened in our laboratory. The X-ray photoelectron spectroscopy (XPS) technique was used to characterize the chemical composition of the surface, and the scanning electronic microscope (SEM) technique was used to perform topographic surface evaluation. Cell cultures were also performed on both surfaces. (3) Results. The superficial chemical analysis of the studied samples presented the following components, approximately, expressed in atomic percentage: O: 39%; Ti: 18%; C: 39%; N: 2%; and Si: 1%. In the same way, the topographic analysis values were obtained in the evaluated roughness parameters: R(a): 1.5 μm ± 0.02%; R(q): 1.31 μm ± 0.33; R(z): 8.98 μm ± 0.73; R(p): 5.12 μm ± 0.48; R(v): 3.76 μm ± 0.51; and R(c): 4.92 μm ± 0.24. At a biological level, the expression of osteocalcin was higher (p < 0.05) on the micro-rough surface compared to that machined at 48 and 96 h of culture. (4) Conclusions. The data obtained in our study indicate that the total carbon content, the relative concentration of titanium, and the roughness of the treatment performed on the implants are in agreement with those found in the literature. Further, the roughness of the treatment performed on the implants throws a spongy, three-dimensional surface suitable for bone growth on it. The biological results found are compatible with the clinical use of the surface tested. |
format | Online Article Text |
id | pubmed-6306932 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2018 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-63069322019-01-02 Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma Rizo-Gorrita, María Luna-Oliva, Irene Serrera-Figallo, María-Angeles Torres-Lagares, Daniel J Funct Biomater Article (1) Background. Titanium is characterized by its biocompatibility, resistance to maximum stress, and fatigue and non-toxicity. The composition, surface structure, and roughness of titanium have a key and direct influence on the osseointegration processes when it is used in the form of dental implants. The objective of the present study is to characterize, at chemical, superficial, and biological levels, the result of the application of the sandblasted with large-grit and acid-etched (SLA) treatment consisting of coarse-grained and double-passivated acid blasting with subsequent decontamination with argon plasma on the surface of titanium implants type IV. (2) Methods. Four Oxtein(®) dental implants (Zaragoza, Spain) were investigated with the following coding: Code L63713T (titanium grade IV, 3.75 mm in diameter, and 13 mm in length). The surface of the implants was SLA type obtained from coarse-grained, double passivated acid, and decontaminated with argon plasma. The samples were in their sealed packages and were opened in our laboratory. The X-ray photoelectron spectroscopy (XPS) technique was used to characterize the chemical composition of the surface, and the scanning electronic microscope (SEM) technique was used to perform topographic surface evaluation. Cell cultures were also performed on both surfaces. (3) Results. The superficial chemical analysis of the studied samples presented the following components, approximately, expressed in atomic percentage: O: 39%; Ti: 18%; C: 39%; N: 2%; and Si: 1%. In the same way, the topographic analysis values were obtained in the evaluated roughness parameters: R(a): 1.5 μm ± 0.02%; R(q): 1.31 μm ± 0.33; R(z): 8.98 μm ± 0.73; R(p): 5.12 μm ± 0.48; R(v): 3.76 μm ± 0.51; and R(c): 4.92 μm ± 0.24. At a biological level, the expression of osteocalcin was higher (p < 0.05) on the micro-rough surface compared to that machined at 48 and 96 h of culture. (4) Conclusions. The data obtained in our study indicate that the total carbon content, the relative concentration of titanium, and the roughness of the treatment performed on the implants are in agreement with those found in the literature. Further, the roughness of the treatment performed on the implants throws a spongy, three-dimensional surface suitable for bone growth on it. The biological results found are compatible with the clinical use of the surface tested. MDPI 2018-12-11 /pmc/articles/PMC6306932/ /pubmed/30544972 http://dx.doi.org/10.3390/jfb9040071 Text en © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Rizo-Gorrita, María Luna-Oliva, Irene Serrera-Figallo, María-Angeles Torres-Lagares, Daniel Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma |
title | Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma |
title_full | Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma |
title_fullStr | Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma |
title_full_unstemmed | Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma |
title_short | Superficial Characteristics of Titanium after Treatment of Chorreated Surface, Passive Acid, and Decontamination with Argon Plasma |
title_sort | superficial characteristics of titanium after treatment of chorreated surface, passive acid, and decontamination with argon plasma |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6306932/ https://www.ncbi.nlm.nih.gov/pubmed/30544972 http://dx.doi.org/10.3390/jfb9040071 |
work_keys_str_mv | AT rizogorritamaria superficialcharacteristicsoftitaniumaftertreatmentofchorreatedsurfacepassiveacidanddecontaminationwithargonplasma AT lunaolivairene superficialcharacteristicsoftitaniumaftertreatmentofchorreatedsurfacepassiveacidanddecontaminationwithargonplasma AT serrerafigallomariaangeles superficialcharacteristicsoftitaniumaftertreatmentofchorreatedsurfacepassiveacidanddecontaminationwithargonplasma AT torreslagaresdaniel superficialcharacteristicsoftitaniumaftertreatmentofchorreatedsurfacepassiveacidanddecontaminationwithargonplasma |