P-S-N Curve Description of Laser Metal Deposition Ti-6.5Al-2Zr-1Mo-1V Titanium Alloy after Duplex Annealing

Fatigue tests were conducted on standard smooth laser metal deposition (LMD) Ti-6.5Al-2Zr-1Mo-1V titanium alloy specimens under three constant-amplitude stresses. The mixed failure behaviors and the influence of internal pores on the fatigue life were discussed in detail. The double-peak characteris...

Descripción completa

Detalles Bibliográficos
Autores principales: Wang, Tianshuai, He, Xiaofan, Wang, Xiaobo, Li, Yuhai
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6384759/
https://www.ncbi.nlm.nih.gov/pubmed/30704044
http://dx.doi.org/10.3390/ma12030418
Descripción
Sumario:Fatigue tests were conducted on standard smooth laser metal deposition (LMD) Ti-6.5Al-2Zr-1Mo-1V titanium alloy specimens under three constant-amplitude stresses. The mixed failure behaviors and the influence of internal pores on the fatigue life were discussed in detail. The double-peak characteristics of the fatigue life distribution have been observed, and a bimodal lognormal distribution (BLG) with five variables can be used to describe the fatigue life variation. A parameter estimation method based on the maximum likelihood estimation (MLE) method was proposed to estimate the BLG distribution parameters, and the Newton–Raphson algorithm was used to solve the nonlinear equations derived from the likelihood functions. A P-S-N curve description of LMD titanium alloy was established based on the BLG and verified by fatigue life data obtained from a fatigue test.