P-S-N Curve Description of Laser Metal Deposition Ti-6.5Al-2Zr-1Mo-1V Titanium Alloy after Duplex Annealing

Fatigue tests were conducted on standard smooth laser metal deposition (LMD) Ti-6.5Al-2Zr-1Mo-1V titanium alloy specimens under three constant-amplitude stresses. The mixed failure behaviors and the influence of internal pores on the fatigue life were discussed in detail. The double-peak characteris...