Effect of Surface Cleaning Regimen on Glass Ceramic Bond Strength

This study investigated the effect of saliva contamination on chemical changes of ceramic surface as well as the influence of saliva cleaning methods on ceramic-resin bond strength. Saliva was used to contaminate leucite (LGC) and lithium disilicate (LDGC) glass ceramic surfaces. The following clean...

Descripción completa

Detalles Bibliográficos
Autores principales: Lapinska, Barbara, Rogowski, Jacek, Nowak, Joanna, Nissan, Joseph, Sokolowski, Jerzy, Lukomska-Szymanska, Monika
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6385042/
https://www.ncbi.nlm.nih.gov/pubmed/30678247
http://dx.doi.org/10.3390/molecules24030389
Descripción
Sumario:This study investigated the effect of saliva contamination on chemical changes of ceramic surface as well as the influence of saliva cleaning methods on ceramic-resin bond strength. Saliva was used to contaminate leucite (LGC) and lithium disilicate (LDGC) glass ceramic surfaces. The following cleaning methods were tested: water spray, cleaning with orthophosphoric acid, universal cleaning paste, ultrasonic cleaning with water, re-etching with hydrofluoric acid. Non-contaminated ceramic sample served as control. Chemical analysis of ceramic surfaces was performed using time-of-flight secondary ion mass spectrometry (TOF-SIMS). Shear bond strength (SBS) of ceramics to resin material was tested after 24-hour water storage and after thermocycling. The most effective cleaning method of saliva-contaminated ceramic surface was cleaning LGC surface with orthophosphoric acid or re-etching the LDGC surface with hydrofluoric acid. The application of the following methods resulted in obtaining reliable bond strength.