Preparation of PVDF/PAR Composites with Piezoelectric Properties by Post-Treatment
Thermoplastic composites were prepared using poly (vinylidene fluoride) (PVDF) as the matrix with piezoelectric properties and aromatic polyarylate (PAR) as the reinforcing component. The PVDF/PAR conjugate fibers were prepared by melt conjugate spinning. The PVDF/PAR composites were prepared by com...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6401780/ https://www.ncbi.nlm.nih.gov/pubmed/30961258 http://dx.doi.org/10.3390/polym10121333 |
Sumario: | Thermoplastic composites were prepared using poly (vinylidene fluoride) (PVDF) as the matrix with piezoelectric properties and aromatic polyarylate (PAR) as the reinforcing component. The PVDF/PAR conjugate fibers were prepared by melt conjugate spinning. The PVDF/PAR composites were prepared by compression molding of the PVDF/PAR conjugate fiber laminates at various molding temperatures. Drawing and poling post-treatments of the PVDF/PAR composites were performed to increase the β crystalline phase content of the PVDF. The morphologies of the PVDF/PAR composites were observed by scanning electron microscopy, and the tensile properties were tested using an universal testing machine. The crystal structure of the PVDF/PAR composites was confirmed by Fourier transform infrared spectroscopy and X-ray diffraction. The piezoelectric properties were tested using voltmeters and multimeters. The post-treatments enhanced the content of the β crystalline phase of the PVDF matrix, thereby improving the piezoelectric properties of the composites. A molding temperature of 180 °C, drawing temperature of 90 °C, and poling voltage of 12 kV were identified as the optimal conditions for the preparation of the PVDF/PAR composite. |
---|