Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide
To assess the potential use of polyamide (PA) for solar-thermal systems applications, the effect of water with varying chlorine content on the fatigue crack growth (FCG) resistance of two PA formulations differing in their stabilizer packages was investigated at 80 °C. A commercial PA containing 30...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6403554/ https://www.ncbi.nlm.nih.gov/pubmed/30960754 http://dx.doi.org/10.3390/polym10080829 |
_version_ | 1783400635456028672 |
---|---|
author | Fischer, Joerg Bradler, Patrick R. Akhras, Mohamad H. Wallner, Gernot M. Lang, Reinhold W. |
author_facet | Fischer, Joerg Bradler, Patrick R. Akhras, Mohamad H. Wallner, Gernot M. Lang, Reinhold W. |
author_sort | Fischer, Joerg |
collection | PubMed |
description | To assess the potential use of polyamide (PA) for solar-thermal systems applications, the effect of water with varying chlorine content on the fatigue crack growth (FCG) resistance of two PA formulations differing in their stabilizer packages was investigated at 80 °C. A commercial PA containing 30 wt % glass fibers and a standard stabilization package (PA-0) was used as the reference material. For the other formulation, the reference material PA-0 was compounded with two additional stabilizers (PA-S1). Keeping the specimen geometry and initial loading conditions the same, the total number of cycles to ultimate specimen failure was found to be reduced with an increase in chlorine content for both materials. As to the effect of the chlorine content on crack growth kinetics, the most pronounced effect in enhancing the crack growth rates or decreasing the FCG resistance was determined between 0 ppm and 1 ppm chlorine content. When comparing the relative change of FCG resistance in chlorinated water (10 ppm) to the FCG resistance in non-chlorinated water (0 ppm), the additional stabilization in the material PA-S1 appears beneficial over the stabilization in the reference material PA-0. |
format | Online Article Text |
id | pubmed-6403554 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2018 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-64035542019-04-02 Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide Fischer, Joerg Bradler, Patrick R. Akhras, Mohamad H. Wallner, Gernot M. Lang, Reinhold W. Polymers (Basel) Article To assess the potential use of polyamide (PA) for solar-thermal systems applications, the effect of water with varying chlorine content on the fatigue crack growth (FCG) resistance of two PA formulations differing in their stabilizer packages was investigated at 80 °C. A commercial PA containing 30 wt % glass fibers and a standard stabilization package (PA-0) was used as the reference material. For the other formulation, the reference material PA-0 was compounded with two additional stabilizers (PA-S1). Keeping the specimen geometry and initial loading conditions the same, the total number of cycles to ultimate specimen failure was found to be reduced with an increase in chlorine content for both materials. As to the effect of the chlorine content on crack growth kinetics, the most pronounced effect in enhancing the crack growth rates or decreasing the FCG resistance was determined between 0 ppm and 1 ppm chlorine content. When comparing the relative change of FCG resistance in chlorinated water (10 ppm) to the FCG resistance in non-chlorinated water (0 ppm), the additional stabilization in the material PA-S1 appears beneficial over the stabilization in the reference material PA-0. MDPI 2018-07-27 /pmc/articles/PMC6403554/ /pubmed/30960754 http://dx.doi.org/10.3390/polym10080829 Text en © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Fischer, Joerg Bradler, Patrick R. Akhras, Mohamad H. Wallner, Gernot M. Lang, Reinhold W. Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide |
title | Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide |
title_full | Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide |
title_fullStr | Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide |
title_full_unstemmed | Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide |
title_short | Influence of Hot Chlorinated Water and Stabilizer Package on the Fatigue Crack Growth Resistance of Glass Fiber Reinforced Polyamide |
title_sort | influence of hot chlorinated water and stabilizer package on the fatigue crack growth resistance of glass fiber reinforced polyamide |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6403554/ https://www.ncbi.nlm.nih.gov/pubmed/30960754 http://dx.doi.org/10.3390/polym10080829 |
work_keys_str_mv | AT fischerjoerg influenceofhotchlorinatedwaterandstabilizerpackageonthefatiguecrackgrowthresistanceofglassfiberreinforcedpolyamide AT bradlerpatrickr influenceofhotchlorinatedwaterandstabilizerpackageonthefatiguecrackgrowthresistanceofglassfiberreinforcedpolyamide AT akhrasmohamadh influenceofhotchlorinatedwaterandstabilizerpackageonthefatiguecrackgrowthresistanceofglassfiberreinforcedpolyamide AT wallnergernotm influenceofhotchlorinatedwaterandstabilizerpackageonthefatiguecrackgrowthresistanceofglassfiberreinforcedpolyamide AT langreinholdw influenceofhotchlorinatedwaterandstabilizerpackageonthefatiguecrackgrowthresistanceofglassfiberreinforcedpolyamide |