Cargando…

Coupled Hygro-Mechanical Finite Element Method on Determination of the Interlaminar Shear Modulus of Glass Fiber-Reinforced Polymer Laminates in Bridge Decks under Hygrothermal Aging Effects

To investigate the mechanical degradation of the shear properties of glass fiber-reinforced polymer (GFRP) laminates in bridge decks under hygrothermal aging effects, short-beam shear tests were performed following the ASTM test standard (ASTM D790-10A). Based on the coupled hygro-mechanical finite...

Descripción completa

Detalles Bibliográficos
Autores principales: Jiang, Xu, Luo, Chengwei, Qiang, Xuhong, Zhang, Qilin, Kolstein, Henk, Bijlaard, Frans
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6403960/
https://www.ncbi.nlm.nih.gov/pubmed/30960770
http://dx.doi.org/10.3390/polym10080845
Descripción
Sumario:To investigate the mechanical degradation of the shear properties of glass fiber-reinforced polymer (GFRP) laminates in bridge decks under hygrothermal aging effects, short-beam shear tests were performed following the ASTM test standard (ASTM D790-10A). Based on the coupled hygro-mechanical finite element (FE) analysis method, an inverse parameter identification approach based on short-beam shear tests was developed and then employed to determine the environment-dependent interlaminar shear modulus of GFRP laminates. Subsequently, the shear strength and modulus of dry (0% M(t)/M(∞)), moisture unsaturated (30% M(t)/M(∞) and 50% M(t)/M(∞)), and moisture saturated (100% M(t)/M(∞)) specimens at test temperatures of both 20 °C and 40 °C were compared. One cycle of the moisture absorption–desorption process was also investigated to address how the moisture-induced residual damage degrades the shear properties of GFRP laminates. The results revealed that the shear strength and modulus of moisture-saturated GFRP laminates decreased significantly, and the elevated testing temperature (40 °C) aggravated moisture-induced mechanical degradation. Moreover, an unrecoverable loss of shear properties for the GFRP laminates enduring one cycle of the moisture absorption–desorption process was evident.