Phase Morphology of NR/SBR Blends: Effect of Curing Temperature and Curing Time

The morphology of natural rubber/styrene–butadiene rubber blends (NR/SBR) was characterized by atomic force microscopy (AFM), with regard to curing temperature and curing time. The changes in blend morphology were directly visualized by AFM which confirmed the results of indirect experiments like di...

Descripción completa

Detalles Bibliográficos
Autores principales: Klat, Darja, Karimi-Varzaneh, Hossein Ali, Lacayo-Pineda, Jorge
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6415377/
https://www.ncbi.nlm.nih.gov/pubmed/30966544
http://dx.doi.org/10.3390/polym10050510
Descripción
Sumario:The morphology of natural rubber/styrene–butadiene rubber blends (NR/SBR) was characterized by atomic force microscopy (AFM), with regard to curing temperature and curing time. The changes in blend morphology were directly visualized by AFM which confirmed the results of indirect experiments like differential scanning calorimetry (DSC). Comparing the phase morphologies at different curing temperatures indicated that the domain size of SBR increases with temperature at lower curing temperatures, but domain growing stops at the latest scorch time. This effect is explained by longer scorch times at low curing temperatures which facilitate phase separation, while the short scorch times at higher temperatures meant that the coalescence of SBR phases was hindered by cross-linking between polymer chains.