Ordered Domains and Microwave Properties of Sub-micron Structured Ba(Zn(1/3)Ta(2/3))O(3) Ceramics Obtained by Spark Plasma Sintering

The degree of Zn(2+) and Ta(5+) ions ordering could play an important role in the dielectric loss in Ba(Zn(1/3)Ta(2/3))O(3) (BZT) ceramics. However, the influence of the grain size of Ba(B′(1/3)B″(2/3))O(3) ceramics with nano or sub-micron grains on the ordering domains structure is still not clear....

Descripción completa

Detalles Bibliográficos
Autores principales: Liu, Fei, Liu, Shaojun, Cui, Xuejiao, Cheng, Lijin, Li, Hao, Wang, Jie, Rao, Weidong
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6419716/
https://www.ncbi.nlm.nih.gov/pubmed/30791626
http://dx.doi.org/10.3390/ma12040638
Descripción
Sumario:The degree of Zn(2+) and Ta(5+) ions ordering could play an important role in the dielectric loss in Ba(Zn(1/3)Ta(2/3))O(3) (BZT) ceramics. However, the influence of the grain size of Ba(B′(1/3)B″(2/3))O(3) ceramics with nano or sub-micron grains on the ordering domains structure is still not clear. In the present paper, highly dense (~98%) BZT microwave dielectric ceramics with homogeneous sub-micron structure (~330 nm) were prepared through spark plasma sintering (SPS). High resolution transmission electron microscopy combined with X-ray diffraction (XRD)clearly showed that the B-site ordering structure of sintered BZT samples by SPS becomes the B-site long-range 1:2 ordering as annealing proceeds. In contrast, the short-range 1:2 ordering in non-annealed counterparts was also present, which was not detectable by XRD. The size of B-site ordering domains enlarged with annealing temperature. The sub-micron structure of sintered BZT ceramics by SPS remained stable at up to 1400 C; however, the size of B-site 1:2 ordering domain was more than five times larger, which led to a significant increase of the quality factor (Q·f) to 37,700 GHz from 15,000 GHz.