Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser

OBJECTIVES: This work presents laser coating of grade 1 pure titanium (Ti) dental implant surface with sintered biological apatite beta-tricalcium phosphate (β-TCP), which has a chemical composition close to bone. MATERIALS AND METHODS: Pulsed Nd:YAG laser of single pulse capability up to 70 J/10 ms...

Descripción completa

Detalles Bibliográficos
Autores principales: Safi, Ihab Nabeel, Hussein, Basima Mohammed Ali, Al Shammari, Ahmed Majeed, Tawfiq, Thaier Abid
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Elsevier 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6445442/
https://www.ncbi.nlm.nih.gov/pubmed/30983835
http://dx.doi.org/10.1016/j.sdentj.2018.12.004
_version_ 1783408195278995456
author Safi, Ihab Nabeel
Hussein, Basima Mohammed Ali
Al Shammari, Ahmed Majeed
Tawfiq, Thaier Abid
author_facet Safi, Ihab Nabeel
Hussein, Basima Mohammed Ali
Al Shammari, Ahmed Majeed
Tawfiq, Thaier Abid
author_sort Safi, Ihab Nabeel
collection PubMed
description OBJECTIVES: This work presents laser coating of grade 1 pure titanium (Ti) dental implant surface with sintered biological apatite beta-tricalcium phosphate (β-TCP), which has a chemical composition close to bone. MATERIALS AND METHODS: Pulsed Nd:YAG laser of single pulse capability up to 70 J/10 ms and pulse peak power of 8 kW was used to implement the task. Laser pulse peak power, pulse duration, repetition rate and scanning speed were modulated to achieve the most homogenous, cohesive and highly adherent coat layer. Scanning electron microscopy (SEM), energy dispersive X-ray microscopy (EDX), optical microscopy and nanoindentation analyses were conducted to characterise and evaluate the microstructure, phases, modulus of elasticity of the coating layer and calcium-to-phosphate ratio and composition. Results showed that the laser power and scanning speed influenced coating adherence. The cross-sectional field-emission scanning electron microscopy images at low power and high speed showed poor adherence and improved as the laser power increased to 2 kW. Decreasing the scanning speed to 0.2 mm/s at the same power of 2 kW increased adherence. EDX results of the substrate demonstrated that the chemical composition of the coat layer did not change after processing. Moreover, the maps revealed proper distribution of Ca and P with some agglomeration on the surface. The sharp peaks on the X-ray diffraction patterns indicated that β-TCPs in the coat layer were mostly crystalline. The elastic modulus was low at the surface and increased gradually with depth to reach 19 GPa at 200 nm; this value was close to that of bone. The microhardness of the coated substrate increased by about 88%. The laser pulse energy of 8.3 J, pulse peak power of 2 kW, pulse duration of 4.3 min, repetition rate of 10 Hz and scanning speed of 0.2 ms(−1) yielded the best results. CONCLUSION: Both processing and coating have potential use for dental implant applications.
format Online
Article
Text
id pubmed-6445442
institution National Center for Biotechnology Information
language English
publishDate 2019
publisher Elsevier
record_format MEDLINE/PubMed
spelling pubmed-64454422019-04-12 Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser Safi, Ihab Nabeel Hussein, Basima Mohammed Ali Al Shammari, Ahmed Majeed Tawfiq, Thaier Abid Saudi Dent J Article OBJECTIVES: This work presents laser coating of grade 1 pure titanium (Ti) dental implant surface with sintered biological apatite beta-tricalcium phosphate (β-TCP), which has a chemical composition close to bone. MATERIALS AND METHODS: Pulsed Nd:YAG laser of single pulse capability up to 70 J/10 ms and pulse peak power of 8 kW was used to implement the task. Laser pulse peak power, pulse duration, repetition rate and scanning speed were modulated to achieve the most homogenous, cohesive and highly adherent coat layer. Scanning electron microscopy (SEM), energy dispersive X-ray microscopy (EDX), optical microscopy and nanoindentation analyses were conducted to characterise and evaluate the microstructure, phases, modulus of elasticity of the coating layer and calcium-to-phosphate ratio and composition. Results showed that the laser power and scanning speed influenced coating adherence. The cross-sectional field-emission scanning electron microscopy images at low power and high speed showed poor adherence and improved as the laser power increased to 2 kW. Decreasing the scanning speed to 0.2 mm/s at the same power of 2 kW increased adherence. EDX results of the substrate demonstrated that the chemical composition of the coat layer did not change after processing. Moreover, the maps revealed proper distribution of Ca and P with some agglomeration on the surface. The sharp peaks on the X-ray diffraction patterns indicated that β-TCPs in the coat layer were mostly crystalline. The elastic modulus was low at the surface and increased gradually with depth to reach 19 GPa at 200 nm; this value was close to that of bone. The microhardness of the coated substrate increased by about 88%. The laser pulse energy of 8.3 J, pulse peak power of 2 kW, pulse duration of 4.3 min, repetition rate of 10 Hz and scanning speed of 0.2 ms(−1) yielded the best results. CONCLUSION: Both processing and coating have potential use for dental implant applications. Elsevier 2019-04 2019-01-08 /pmc/articles/PMC6445442/ /pubmed/30983835 http://dx.doi.org/10.1016/j.sdentj.2018.12.004 Text en © 2019 The Authors http://creativecommons.org/licenses/by-nc-nd/4.0/ This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
spellingShingle Article
Safi, Ihab Nabeel
Hussein, Basima Mohammed Ali
Al Shammari, Ahmed Majeed
Tawfiq, Thaier Abid
Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser
title Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser
title_full Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser
title_fullStr Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser
title_full_unstemmed Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser
title_short Implementation and characterization of coating pure titanium dental implant with sintered β-TCP by using Nd:YAG laser
title_sort implementation and characterization of coating pure titanium dental implant with sintered β-tcp by using nd:yag laser
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6445442/
https://www.ncbi.nlm.nih.gov/pubmed/30983835
http://dx.doi.org/10.1016/j.sdentj.2018.12.004
work_keys_str_mv AT safiihabnabeel implementationandcharacterizationofcoatingpuretitaniumdentalimplantwithsinteredbtcpbyusingndyaglaser
AT husseinbasimamohammedali implementationandcharacterizationofcoatingpuretitaniumdentalimplantwithsinteredbtcpbyusingndyaglaser
AT alshammariahmedmajeed implementationandcharacterizationofcoatingpuretitaniumdentalimplantwithsinteredbtcpbyusingndyaglaser
AT tawfiqthaierabid implementationandcharacterizationofcoatingpuretitaniumdentalimplantwithsinteredbtcpbyusingndyaglaser