The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments
The intergranular corrosion (IGC) behavior of a new metastable austenitic Cr–Mn–Ni–N–Cu high-strength stainless steel under various heat treatments was studied. The samples were solution treated at 1050 °C for 30 min and then aged at 600 to 900 °C for 10 to 300 min, respectively. The IGC susceptibil...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2019
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6539159/ https://www.ncbi.nlm.nih.gov/pubmed/31035439 http://dx.doi.org/10.3390/ma12091385 |
_version_ | 1783422320022388736 |
---|---|
author | Liu, Guangming Liu, Yuanyuan Cheng, Yawen Li, Jin Jiang, Yiming |
author_facet | Liu, Guangming Liu, Yuanyuan Cheng, Yawen Li, Jin Jiang, Yiming |
author_sort | Liu, Guangming |
collection | PubMed |
description | The intergranular corrosion (IGC) behavior of a new metastable austenitic Cr–Mn–Ni–N–Cu high-strength stainless steel under various heat treatments was studied. The samples were solution treated at 1050 °C for 30 min and then aged at 600 to 900 °C for 10 to 300 min, respectively. The IGC susceptibility of aged samples was investigated using a double-loop electrochemical potentiokinetic reactivation (DL-EPR) test in a solution of 0.1 M H(2)SO(4) and 0.002 M KSCN and the 10% oxalic acid etch. The surface morphologies of samples were characterized using optical microscopy and the scanning electron microscopy after electrochemical tests. Two time-temperature-sensitization diagrams were plotted based on the DL-EPR test and oxalic acid etching. No IGC and precipitate were observed for samples aged at 600 °C and 900 °C. For samples aged at 650 °C to 750 °C, the IGC susceptibility and the amount of precipitate both increased with the extended aging time. For samples aged at 800 °C and 850 °C, the amount of precipitate increased as the aging time was prolonged. However, only the sample aged at 800 °C for 60 min showed slight intergranular corrosion in the DL-EPR test. The IGC of the Cr–Mn–Ni–N–Cu austenitic stainless steel originated from the precipitation of Cr(23)C(6) and Cr(2)N at the grain boundaries. The chromium-depleted zones near grain boundaries stood as the corrosion nucleation sites, but the dissolution of the weak area followed a consistent crystallographic orientation along each grain boundary. |
format | Online Article Text |
id | pubmed-6539159 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2019 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-65391592019-06-05 The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments Liu, Guangming Liu, Yuanyuan Cheng, Yawen Li, Jin Jiang, Yiming Materials (Basel) Article The intergranular corrosion (IGC) behavior of a new metastable austenitic Cr–Mn–Ni–N–Cu high-strength stainless steel under various heat treatments was studied. The samples were solution treated at 1050 °C for 30 min and then aged at 600 to 900 °C for 10 to 300 min, respectively. The IGC susceptibility of aged samples was investigated using a double-loop electrochemical potentiokinetic reactivation (DL-EPR) test in a solution of 0.1 M H(2)SO(4) and 0.002 M KSCN and the 10% oxalic acid etch. The surface morphologies of samples were characterized using optical microscopy and the scanning electron microscopy after electrochemical tests. Two time-temperature-sensitization diagrams were plotted based on the DL-EPR test and oxalic acid etching. No IGC and precipitate were observed for samples aged at 600 °C and 900 °C. For samples aged at 650 °C to 750 °C, the IGC susceptibility and the amount of precipitate both increased with the extended aging time. For samples aged at 800 °C and 850 °C, the amount of precipitate increased as the aging time was prolonged. However, only the sample aged at 800 °C for 60 min showed slight intergranular corrosion in the DL-EPR test. The IGC of the Cr–Mn–Ni–N–Cu austenitic stainless steel originated from the precipitation of Cr(23)C(6) and Cr(2)N at the grain boundaries. The chromium-depleted zones near grain boundaries stood as the corrosion nucleation sites, but the dissolution of the weak area followed a consistent crystallographic orientation along each grain boundary. MDPI 2019-04-29 /pmc/articles/PMC6539159/ /pubmed/31035439 http://dx.doi.org/10.3390/ma12091385 Text en © 2019 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Liu, Guangming Liu, Yuanyuan Cheng, Yawen Li, Jin Jiang, Yiming The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments |
title | The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments |
title_full | The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments |
title_fullStr | The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments |
title_full_unstemmed | The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments |
title_short | The Intergranular Corrosion Susceptibility of Metastable Austenitic Cr–Mn–Ni–N–Cu High-Strength Stainless Steel under Various Heat Treatments |
title_sort | intergranular corrosion susceptibility of metastable austenitic cr–mn–ni–n–cu high-strength stainless steel under various heat treatments |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6539159/ https://www.ncbi.nlm.nih.gov/pubmed/31035439 http://dx.doi.org/10.3390/ma12091385 |
work_keys_str_mv | AT liuguangming theintergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT liuyuanyuan theintergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT chengyawen theintergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT lijin theintergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT jiangyiming theintergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT liuguangming intergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT liuyuanyuan intergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT chengyawen intergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT lijin intergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments AT jiangyiming intergranularcorrosionsusceptibilityofmetastableausteniticcrmnnincuhighstrengthstainlesssteelundervariousheattreatments |