Temperature Stable Cold Sintered (Bi(0.95)Li(0.05))(V(0.9)Mo(0.1))O(4)-Na(2)Mo(2)O(7) Microwave Dielectric Composites
Dense (Bi(0.95)Li(0.05))(V(0.9)Mo(0.1))O(4)-Na(2)Mo(2)O(7) (100−x) wt.% (Bi(0.95)Li(0.05))(V(0.9)Mo(0.1))O(4) (BLVMO)-x wt.% Na(2)Mo(2)O(7) (NMO) composite ceramics were successfully fabricated through cold sintering at 150 °C under at 200 MPa for 30 min. X-ray diffraction, back-scattered scanning e...