Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy

Ni, Co, Mg, and Al mixed-oxide solids, synthesized via the hydrotalcite route, were investigated in previous works toward the dry reforming of methane for hydrogen production. The oxide Co(2)Ni(2)Mg(2)Al(2) calcined at 800 °C, Co(2)Ni(2)Mg(2)Al(2)800, showed the highest catalytic activity in the stu...

Descripción completa

Detalles Bibliográficos
Autores principales: Tanios, Carole, Gennequin, Cédric, Labaki, Madona, Tidahy, Haingomalala Lucette, Aboukaïs, Antoine, Abi-Aad, Edmond
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6540188/
https://www.ncbi.nlm.nih.gov/pubmed/31027355
http://dx.doi.org/10.3390/ma12091362
_version_ 1783422563325575168
author Tanios, Carole
Gennequin, Cédric
Labaki, Madona
Tidahy, Haingomalala Lucette
Aboukaïs, Antoine
Abi-Aad, Edmond
author_facet Tanios, Carole
Gennequin, Cédric
Labaki, Madona
Tidahy, Haingomalala Lucette
Aboukaïs, Antoine
Abi-Aad, Edmond
author_sort Tanios, Carole
collection PubMed
description Ni, Co, Mg, and Al mixed-oxide solids, synthesized via the hydrotalcite route, were investigated in previous works toward the dry reforming of methane for hydrogen production. The oxide Co(2)Ni(2)Mg(2)Al(2) calcined at 800 °C, Co(2)Ni(2)Mg(2)Al(2)800, showed the highest catalytic activity in the studied series, which was ascribable to an interaction between Ni and Co, which is optimal for this Co/Ni ratio. In the present study, Co(2)Ni(2)Mg(2)Al(2)800 was compared to a commercial catalyst widely used in the industry, Ni(50%)/Al(2)O(3), and showed better activity despite its lower number of active sites, as well as lower amounts of carbon on its surface, i.e. less deactivation. In addition to this, Co(2)Ni(2)Mg(2)Al(2)800 showed stability for 20 h under stream during the dry reforming of methane. This good durability is attributed to a periodic cycle of carbon deposition and removal as well as to the strong interaction between Ni and Co, preventing the deactivation of the catalyst. The evaluation of the catalytic performances in the presence of toluene, which is an impurity that exists in biogas, is also a part of this work. In the presence of toluene, the catalytic activity of Co(2)Ni(2)Mg(2)Al(2)800 decreases, and higher carbon formation on the catalyst surface is detected. Toluene adsorption on catalytic sites, side reactions performed by toluene, and the competition between toluene and methane in the reaction with carbon dioxide are the main reasons for such results.
format Online
Article
Text
id pubmed-6540188
institution National Center for Biotechnology Information
language English
publishDate 2019
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-65401882019-06-05 Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy Tanios, Carole Gennequin, Cédric Labaki, Madona Tidahy, Haingomalala Lucette Aboukaïs, Antoine Abi-Aad, Edmond Materials (Basel) Article Ni, Co, Mg, and Al mixed-oxide solids, synthesized via the hydrotalcite route, were investigated in previous works toward the dry reforming of methane for hydrogen production. The oxide Co(2)Ni(2)Mg(2)Al(2) calcined at 800 °C, Co(2)Ni(2)Mg(2)Al(2)800, showed the highest catalytic activity in the studied series, which was ascribable to an interaction between Ni and Co, which is optimal for this Co/Ni ratio. In the present study, Co(2)Ni(2)Mg(2)Al(2)800 was compared to a commercial catalyst widely used in the industry, Ni(50%)/Al(2)O(3), and showed better activity despite its lower number of active sites, as well as lower amounts of carbon on its surface, i.e. less deactivation. In addition to this, Co(2)Ni(2)Mg(2)Al(2)800 showed stability for 20 h under stream during the dry reforming of methane. This good durability is attributed to a periodic cycle of carbon deposition and removal as well as to the strong interaction between Ni and Co, preventing the deactivation of the catalyst. The evaluation of the catalytic performances in the presence of toluene, which is an impurity that exists in biogas, is also a part of this work. In the presence of toluene, the catalytic activity of Co(2)Ni(2)Mg(2)Al(2)800 decreases, and higher carbon formation on the catalyst surface is detected. Toluene adsorption on catalytic sites, side reactions performed by toluene, and the competition between toluene and methane in the reaction with carbon dioxide are the main reasons for such results. MDPI 2019-04-26 /pmc/articles/PMC6540188/ /pubmed/31027355 http://dx.doi.org/10.3390/ma12091362 Text en © 2019 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Tanios, Carole
Gennequin, Cédric
Labaki, Madona
Tidahy, Haingomalala Lucette
Aboukaïs, Antoine
Abi-Aad, Edmond
Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy
title Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy
title_full Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy
title_fullStr Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy
title_full_unstemmed Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy
title_short Evaluation of a Catalyst Durability in Absence and Presence of Toluene Impurity: Case of the Material Co(2)Ni(2)Mg(2)Al(2) Mixed Oxide Prepared by Hydrotalcite Route in Methane Dry Reforming to Produce Energy
title_sort evaluation of a catalyst durability in absence and presence of toluene impurity: case of the material co(2)ni(2)mg(2)al(2) mixed oxide prepared by hydrotalcite route in methane dry reforming to produce energy
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6540188/
https://www.ncbi.nlm.nih.gov/pubmed/31027355
http://dx.doi.org/10.3390/ma12091362
work_keys_str_mv AT tanioscarole evaluationofacatalystdurabilityinabsenceandpresenceoftolueneimpuritycaseofthematerialco2ni2mg2al2mixedoxidepreparedbyhydrotalciterouteinmethanedryreformingtoproduceenergy
AT gennequincedric evaluationofacatalystdurabilityinabsenceandpresenceoftolueneimpuritycaseofthematerialco2ni2mg2al2mixedoxidepreparedbyhydrotalciterouteinmethanedryreformingtoproduceenergy
AT labakimadona evaluationofacatalystdurabilityinabsenceandpresenceoftolueneimpuritycaseofthematerialco2ni2mg2al2mixedoxidepreparedbyhydrotalciterouteinmethanedryreformingtoproduceenergy
AT tidahyhaingomalalalucette evaluationofacatalystdurabilityinabsenceandpresenceoftolueneimpuritycaseofthematerialco2ni2mg2al2mixedoxidepreparedbyhydrotalciterouteinmethanedryreformingtoproduceenergy
AT aboukaisantoine evaluationofacatalystdurabilityinabsenceandpresenceoftolueneimpuritycaseofthematerialco2ni2mg2al2mixedoxidepreparedbyhydrotalciterouteinmethanedryreformingtoproduceenergy
AT abiaadedmond evaluationofacatalystdurabilityinabsenceandpresenceoftolueneimpuritycaseofthematerialco2ni2mg2al2mixedoxidepreparedbyhydrotalciterouteinmethanedryreformingtoproduceenergy