Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia

The aim of this study was to evaluate the long term stability of shear bond strength (SBS) when 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) containing universal adhesive was used in the ceramic bracket bonding on dental zirconia. Twenty human maxillary incisors were collected. The ceramic...

Descripción completa

Detalles Bibliográficos
Autores principales: Ju, Ga-Youn, Oh, Soram, Lim, Bum-Soon, Lee, Hyun-Seung, Chung, Shin Hye
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6566336/
https://www.ncbi.nlm.nih.gov/pubmed/31137486
http://dx.doi.org/10.3390/ma12101640
_version_ 1783426828934840320
author Ju, Ga-Youn
Oh, Soram
Lim, Bum-Soon
Lee, Hyun-Seung
Chung, Shin Hye
author_facet Ju, Ga-Youn
Oh, Soram
Lim, Bum-Soon
Lee, Hyun-Seung
Chung, Shin Hye
author_sort Ju, Ga-Youn
collection PubMed
description The aim of this study was to evaluate the long term stability of shear bond strength (SBS) when 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) containing universal adhesive was used in the ceramic bracket bonding on dental zirconia. Twenty human maxillary incisors were collected. The ceramic bracket was bonded on the buccal enamel surface after the acid-etching and orthodontic primer application (Group CON). Sixty zirconia specimens were sintered, sandblasted and divided into three experimental groups; group CP—ceramic primer followed by an orthodontic primer; group U—universal adhesive; group CU—ceramic primer followed by a universal adhesive. For each specimen, the bracket was bonded onto the treated surface with composite resin (Transbond XT, 3M ESPE). The SBS tested before (CON0, CP0, U0, CU0) and after the artificial aging (CON1, CP1, U1, CU1). The data were statistically analyzed with the Kruskal–Wallis test at a significance level of 0.05. The mean SBS of CON0, CP0, U0 and CU0 were within the clinically acceptable range without significant differences. After the aging process, SBS decreased in all groups. Among the aged groups, CP1 showed the highest SBS. Based on the results, when bonding ceramic brackets to a dental zirconia surface, we can conclude that ceramic primer used with an orthodontic primer, rather than using a universal adhesive, is recommended.
format Online
Article
Text
id pubmed-6566336
institution National Center for Biotechnology Information
language English
publishDate 2019
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-65663362019-06-17 Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia Ju, Ga-Youn Oh, Soram Lim, Bum-Soon Lee, Hyun-Seung Chung, Shin Hye Materials (Basel) Article The aim of this study was to evaluate the long term stability of shear bond strength (SBS) when 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) containing universal adhesive was used in the ceramic bracket bonding on dental zirconia. Twenty human maxillary incisors were collected. The ceramic bracket was bonded on the buccal enamel surface after the acid-etching and orthodontic primer application (Group CON). Sixty zirconia specimens were sintered, sandblasted and divided into three experimental groups; group CP—ceramic primer followed by an orthodontic primer; group U—universal adhesive; group CU—ceramic primer followed by a universal adhesive. For each specimen, the bracket was bonded onto the treated surface with composite resin (Transbond XT, 3M ESPE). The SBS tested before (CON0, CP0, U0, CU0) and after the artificial aging (CON1, CP1, U1, CU1). The data were statistically analyzed with the Kruskal–Wallis test at a significance level of 0.05. The mean SBS of CON0, CP0, U0 and CU0 were within the clinically acceptable range without significant differences. After the aging process, SBS decreased in all groups. Among the aged groups, CP1 showed the highest SBS. Based on the results, when bonding ceramic brackets to a dental zirconia surface, we can conclude that ceramic primer used with an orthodontic primer, rather than using a universal adhesive, is recommended. MDPI 2019-05-20 /pmc/articles/PMC6566336/ /pubmed/31137486 http://dx.doi.org/10.3390/ma12101640 Text en © 2019 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Ju, Ga-Youn
Oh, Soram
Lim, Bum-Soon
Lee, Hyun-Seung
Chung, Shin Hye
Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia
title Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia
title_full Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia
title_fullStr Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia
title_full_unstemmed Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia
title_short Effect of Simplified Bonding on Shear Bond Strength between Ceramic Brackets and Dental Zirconia
title_sort effect of simplified bonding on shear bond strength between ceramic brackets and dental zirconia
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6566336/
https://www.ncbi.nlm.nih.gov/pubmed/31137486
http://dx.doi.org/10.3390/ma12101640
work_keys_str_mv AT jugayoun effectofsimplifiedbondingonshearbondstrengthbetweenceramicbracketsanddentalzirconia
AT ohsoram effectofsimplifiedbondingonshearbondstrengthbetweenceramicbracketsanddentalzirconia
AT limbumsoon effectofsimplifiedbondingonshearbondstrengthbetweenceramicbracketsanddentalzirconia
AT leehyunseung effectofsimplifiedbondingonshearbondstrengthbetweenceramicbracketsanddentalzirconia
AT chungshinhye effectofsimplifiedbondingonshearbondstrengthbetweenceramicbracketsanddentalzirconia