All-Oxide Thermoelectric Module with in Situ Formed Non-Rectifying Complex p–p–n Junction and Transverse Thermoelectric Effect

[Image: see text] All-oxide thermoelectric modules for energy harvesting are attractive because of high-temperature stability, low cost, and the potential to use nonscarce and nontoxic elements. Thermoelectric modules are mostly fabricated in the conventional π-design, associated with the challenge...

Descripción completa

Detalles Bibliográficos
Autores principales: Kanas, Nikola, Bittner, Michael, Desissa, Temesgen Debelo, Singh, Sathya Prakash, Norby, Truls, Feldhoff, Armin, Grande, Tor, Wiik, Kjell, Einarsrud, Mari-Ann
Formato: Online Artículo Texto
Lenguaje:English
Publicado: American Chemical Society 2018
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6644604/
https://www.ncbi.nlm.nih.gov/pubmed/31459118
http://dx.doi.org/10.1021/acsomega.8b01357
Descripción
Sumario:[Image: see text] All-oxide thermoelectric modules for energy harvesting are attractive because of high-temperature stability, low cost, and the potential to use nonscarce and nontoxic elements. Thermoelectric modules are mostly fabricated in the conventional π-design, associated with the challenge of unstable metallic interconnects at high temperature. Here, we report on a novel approach for fabrication of a thermoelectric module with an in situ formed p–p–n junction made of state-of-the-art oxides Ca(3)Co(4–x)O(9+δ) (p-type) and CaMnO(3)–CaMn(2)O(4) composite (n-type). The module was fabricated by spark plasma co-sintering of p- and n-type powders partly separated by insulating LaAlO(3). Where the n- and p-type materials originally were in contact, a layer of p-type Ca(3)CoMnO(6) was formed in situ. The hence formed p–p–n junction exhibited Ohmic behavior and a transverse thermoelectric effect, boosting the open-circuit voltage of the module. The performance of the module was characterized at 700–900 °C, with the highest power output of 5.7 mW (around 23 mW/cm(2)) at 900 °C and a temperature difference of 160 K. The thermoelectric properties of the p- and n-type materials were measured in the temperature range 100–900 °C, where the highest zT of 0.39 and 0.05 were obtained at 700 and 800 °C, respectively, for Ca(3)Co(4–x)O(9+δ) and the CaMnO(3)–CaMn(2)O(4) composite.