New Findings in Hydrothermal Deactivation Research on the Vanadia-Selective Catalytic Reduction Catalyst
[Image: see text] Considering the risks of hydrothermal deterioration in vehicles, power plants, and oceangoing vessels, V(2)O(5)-WO(3)/TiO(2) catalysts were subject to hydrothermal and thermal aging at 600, 625, 635, and 650 °C for 4–48 h. The different ratio and significant loss of active sites ar...