De-alloying Behavior of Mg–Al alloy in Sulphuric Acid and Acetic Acid Aqueous Solutions
The fabricated Mg–Al alloy consists of α-Mg phase and Mg–Mg(17)Al(12) eutectic phase. The corrosion behavior of cast Mg–Al alloy in sulphuric acid (H(2)SO(4)) and acetic acid (HAc) aqueous solutions was investigated. The Mg–Al alloy shows general corrosion in H(2)SO(4) solution, and the α-Mg dendrit...
Autores principales: | Li, Yonggang, Wei, Yinghui, Yang, Shengqiang |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2019
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6651890/ https://www.ncbi.nlm.nih.gov/pubmed/31247922 http://dx.doi.org/10.3390/ma12132046 |
Ejemplares similares
-
Corrosion Behavior of the As-Cast and As-Solid Solution Mg-Al-Ge Alloy
por: Liu, Xiaoda, et al.
Publicado: (2018) -
Investigation on Wear Behavior of Cryogenically Treated Ti-6Al-4V Titanium Alloy under Dry and Wet Conditions
por: Li, Yonggang, et al.
Publicado: (2019) -
Using real-time UV–visible spectrophotometer to assess an Al–Zn–Mg–Cu alloy's dissolution in acidic solution
por: Sun, Qingqing, et al.
Publicado: (2020) -
Effect of Thermal Treatments on Sn-Alloyed Al-Mg-Si Alloys
por: Schmid, Florian, et al.
Publicado: (2019) -
Aging Behavior and Precipitates Analysis of Wrought Al-Si-Mg Alloy
por: Liu, Fang, et al.
Publicado: (2022)