Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide

Ultrafine grained WC-12Co-0.2VC (named UYG12V) cemented carbides were prepared via the two-step spark plasma sintering (SPS) in this study. First, the effects of the sintering temperature on the relative density and WC grain size of UYG12V cemented carbides were studied. The results show that regula...

Descripción completa

Detalles Bibliográficos
Autores principales: Wang, Zhenhua, Jia, Jiheng, Wang, Boxiang, Wang, Yulin
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6695939/
https://www.ncbi.nlm.nih.gov/pubmed/31370236
http://dx.doi.org/10.3390/ma12152443
_version_ 1783444152685428736
author Wang, Zhenhua
Jia, Jiheng
Wang, Boxiang
Wang, Yulin
author_facet Wang, Zhenhua
Jia, Jiheng
Wang, Boxiang
Wang, Yulin
author_sort Wang, Zhenhua
collection PubMed
description Ultrafine grained WC-12Co-0.2VC (named UYG12V) cemented carbides were prepared via the two-step spark plasma sintering (SPS) in this study. First, the effects of the sintering temperature on the relative density and WC grain size of UYG12V cemented carbides were studied. The results show that regular WC grains form when sintered at 1300 °C. The sintered body begins to rapidly densify and WC grains grow slowly when sintered at 1200 °C. Thus, the first-step (T1) and the second-step (T2) temperatures in the two-step SPS of UYG12V are 1300 °C and 1200 °C, respectively. The effect of the holding time during the first and second steps on the mechanical properties was also studied. The results show that the UYG12V cemented carbide sintered at 1300 °C for 3 min and then at 1200 °C for 5 min has the best comprehensive mechanical properties, exhibiting the average particle size, Vickers hardness, fracture toughness, relative density, and bending strength of 271 nm, 18.06 GPa, 12.25 MPa m(1/2), 99.49%, and 1960 MPa, respectively.
format Online
Article
Text
id pubmed-6695939
institution National Center for Biotechnology Information
language English
publishDate 2019
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-66959392019-09-05 Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide Wang, Zhenhua Jia, Jiheng Wang, Boxiang Wang, Yulin Materials (Basel) Article Ultrafine grained WC-12Co-0.2VC (named UYG12V) cemented carbides were prepared via the two-step spark plasma sintering (SPS) in this study. First, the effects of the sintering temperature on the relative density and WC grain size of UYG12V cemented carbides were studied. The results show that regular WC grains form when sintered at 1300 °C. The sintered body begins to rapidly densify and WC grains grow slowly when sintered at 1200 °C. Thus, the first-step (T1) and the second-step (T2) temperatures in the two-step SPS of UYG12V are 1300 °C and 1200 °C, respectively. The effect of the holding time during the first and second steps on the mechanical properties was also studied. The results show that the UYG12V cemented carbide sintered at 1300 °C for 3 min and then at 1200 °C for 5 min has the best comprehensive mechanical properties, exhibiting the average particle size, Vickers hardness, fracture toughness, relative density, and bending strength of 271 nm, 18.06 GPa, 12.25 MPa m(1/2), 99.49%, and 1960 MPa, respectively. MDPI 2019-07-31 /pmc/articles/PMC6695939/ /pubmed/31370236 http://dx.doi.org/10.3390/ma12152443 Text en © 2019 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Wang, Zhenhua
Jia, Jiheng
Wang, Boxiang
Wang, Yulin
Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide
title Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide
title_full Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide
title_fullStr Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide
title_full_unstemmed Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide
title_short Two-Step Spark Plasma Sintering Process of Ultrafine Grained WC-12Co-0.2VC Cemented Carbide
title_sort two-step spark plasma sintering process of ultrafine grained wc-12co-0.2vc cemented carbide
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6695939/
https://www.ncbi.nlm.nih.gov/pubmed/31370236
http://dx.doi.org/10.3390/ma12152443
work_keys_str_mv AT wangzhenhua twostepsparkplasmasinteringprocessofultrafinegrainedwc12co02vccementedcarbide
AT jiajiheng twostepsparkplasmasinteringprocessofultrafinegrainedwc12co02vccementedcarbide
AT wangboxiang twostepsparkplasmasinteringprocessofultrafinegrainedwc12co02vccementedcarbide
AT wangyulin twostepsparkplasmasinteringprocessofultrafinegrainedwc12co02vccementedcarbide