Effects of Cr, W, and Mo on the High Temperature Oxidation of Ni-Based Superalloys
The oxidation behavior of Ni–9.5Co–(8~12)Cr–(2.5~5.5)Mo–(4~8)W–3Al–5Ti–3Ta–0.1C–0.01B alloys was investigated at 850 °C and 1000 °C The mass change, the phase of oxides, and the cross-sectional structure of specimens were analyzed after cyclic oxidation tests. The oxide scale was composed mainly of...
Autores principales: | Park, Si-Jun, Seo, Seong-Moon, Yoo, Young-Soo, Jeong, Hi-Won, Jang, HeeJin |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2019
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6766203/ https://www.ncbi.nlm.nih.gov/pubmed/31514315 http://dx.doi.org/10.3390/ma12182934 |
Ejemplares similares
-
Effect of Long-Term High Temperature Oxidation on the Coking Behavior of Ni-Cr Superalloys
por: Sarris, Stamatis A., et al.
Publicado: (2018) -
Carbides Evolution in a Ni-16Mo-7Cr Base Superalloy during Long-Term Thermal Exposure
por: Han, Fenfen, et al.
Publicado: (2017) -
The Effects of Alloying Elements Cr, Al, and Si on Oxidation Behaviors of Ni-Based Superalloys
por: Ma, Suyu, et al.
Publicado: (2022) -
Ni–Al–Cr superalloy as high temperature cathode current collector for advanced thin film Li batteries
por: Filippin, Alejandro N., et al.
Publicado: (2018) -
Effect of Ni, W and Mo on the microstructure, phases and high-temperature sliding wear performance of CoCr matrix alloys
por: Cui, Gongjun, et al.
Publicado: (2020)