Enhanced Figure of Merit in Bismuth-Antimony Fine-Grained Alloys at Cryogenic Temperatures

Thermoelectric (TE) materials research plays a vital role in heat-to-electrical energy conversion and refrigeration applications. Bismuth-antimony (Bi-Sb) alloy is a promising material for thermoelectric cooling. Herein, a high figure of merit, ZT, near 0.6 at cryogenic temperatures (100–150 K) has...

Descripción completa

Detalles Bibliográficos
Autores principales: Gao, Sheng, Gaskins, John, Hu, Xixiao, Tomko, Kathleen, Hopkins, Patrick, Poon, S. Joseph
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6797736/
https://www.ncbi.nlm.nih.gov/pubmed/31624277
http://dx.doi.org/10.1038/s41598-019-50325-7
Descripción
Sumario:Thermoelectric (TE) materials research plays a vital role in heat-to-electrical energy conversion and refrigeration applications. Bismuth-antimony (Bi-Sb) alloy is a promising material for thermoelectric cooling. Herein, a high figure of merit, ZT, near 0.6 at cryogenic temperatures (100–150 K) has been achieved in melt-spun n-type Bi(85)Sb(15) bulk samples consisting of micron-size grains. The achieved ZT is nearly 50% higher than polycrystalline averaged single crystal ZT of ~0.4, and it is also significantly higher than ZT of less than ~0.3 measured below 150 K in Bi-Te alloys commonly used for cryogenic cooling applications. The improved thermoelectric properties can be attributed to the fine-grained microstructure achieved from rapid solidification, which not only significantly reduced the thermal conductivity but also mitigated a segregation effect. A record low thermal conductivity of ~1.5 W m(−1) K(−1) near 100 K was measured using the hot disk method. The thermoelectric properties for this intriguing semimetal-semiconductor alloy system were analyzed within a two-band effective mass model. The study revealed a gradual narrowing of the band gap at increasing temperature in Bi-Sb alloy for the first time. Magneto-thermoelectric effects of this Bi-Sb alloy further improved the TE properties, leading to ZT of about 0.7. The magneto-TE effect was further demonstrated in a combined NdFeB/BiSb/NdFeB system. The compactness of the BiSb-magnet system with high ZT enables the utilization of magneto-TE effect in thermoelectric cooling applications.