Emissions of DEHP‐free PVC flooring

Degrading 2‐ethylhexyl‐containing PVC floorings (eg DEHP‐PVC floorings) and adhesives emit 2‐ethylhexanol (2‐EH) in the indoor air. The danger of flooring degradation comes from exposing occupants to harmful phthalates plasticisers (eg DEHP), but not from 2‐EH as such. Since the EU banned the use of...

Descripción completa

Detalles Bibliográficos
Autores principales: Castagnoli, Emmanuelle, Backlund, Peter, Talvitie, Oskari, Tuomi, Tapani, Valtanen, Arja, Mikkola, Raimo, Hovi, Hanna, Leino, Katri, Kurnitski, Jarek, Salonen, Heidi
Formato: Online Artículo Texto
Lenguaje:English
Publicado: John Wiley and Sons Inc. 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6856815/
https://www.ncbi.nlm.nih.gov/pubmed/31348556
http://dx.doi.org/10.1111/ina.12591
Descripción
Sumario:Degrading 2‐ethylhexyl‐containing PVC floorings (eg DEHP‐PVC floorings) and adhesives emit 2‐ethylhexanol (2‐EH) in the indoor air. The danger of flooring degradation comes from exposing occupants to harmful phthalates plasticisers (eg DEHP), but not from 2‐EH as such. Since the EU banned the use of phthalates in sensitive applications, the market is shifting to use DEHP‐free and alternative types of plasticisers in PVC products. However, data on emissions from DEHP‐free PVC floorings are scarce. This study aimed at assessing the surface and bulk emissions of two DEHP‐free PVC floorings over three years. The floorings were glued on the screed layer of concrete casts at 75%, 85%, and 95% RH. The volatile organic compounds (VOCs) were actively sampled using FLEC (surface emissions) and micro‐chamber/thermal extractor (µ‐CTE, bulk emissions) onto Tenax TA adsorbents and analyzed with TD‐GC‐MS. 2‐EH, C9‐alcohols, and total volatile organic compound (TVOC) emissions are reported. Emissions at 75% and 85% RH were similar. As expected, the highest emissions occurred at 95% RH. 2‐EH emissions originated from the adhesive. Because the two DEHP‐free floorings tested emitted C9‐alcohols at all tested RH, it makes the detection of flooring degradation harder, particularly if the adhesive used does not emit 2‐EH.