Preparation, Mechanical Properties, and High-Temperature Wear Resistance of Ti–Al–B alloy

Ti–Al matrix alloy reinforced with a high content of boron was fabricated by using a high-temperature alloying method and powder metallurgy technique (P/M). The preparation method of Ti–Al–B alloying powder was put forward. Phases, microstructure, and mechanical properties of the alloys were investi...

Descripción completa

Detalles Bibliográficos
Autores principales: Cui, Gongjun, Liu, Yanping, Gao, Guijun, Liu, Huiqiang, Li, Sai, Kou, Ziming
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6888182/
https://www.ncbi.nlm.nih.gov/pubmed/31739472
http://dx.doi.org/10.3390/ma12223751
Descripción
Sumario:Ti–Al matrix alloy reinforced with a high content of boron was fabricated by using a high-temperature alloying method and powder metallurgy technique (P/M). The preparation method of Ti–Al–B alloying powder was put forward. Phases, microstructure, and mechanical properties of the alloys were investigated. Wear and friction performance were studied by using a ball-on-disc tribotester sliding against a Si(3)N(4) ceramic ball from 23 °C (room temperature) to 900 °C. The Ti–Al–B alloy had a higher specific strength than that of the Ti–Al alloy. The boron element obviously enhanced the wear resistance and mechanical properties of the alloys because of the formation of borides (TiB(2) and AlB(2)) in matrices and the stable oxide film on the wear tracks. Friction coefficients of alloys were independent of the boron element. The wear mechanisms of the alloys transferred from fatigue wear to oxidative wear with the increase in temperature.