Arginine-Induced Self-Assembly of Protoporphyrin to Obtain Effective Photocatalysts in Aqueous Media Under Visible Light

The fabrication of controlled supramolecular nanostructures via self-assembly of protoporphyrin IX (PPIX) was studied with enantiomerically pure l-arginine and d-arginine, and we have shown that stoichiometry controlled the morphology formed. The nanostructure morphology was mainly influenced by the...

Descripción completa

Detalles Bibliográficos
Autores principales: Aljabri, Mahmood D., Gosavi, Nilesh M., Jones, Lathe A., Morajkar, Pranay P., La, Duong D., Bhosale, Sheshanath V.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6891641/
https://www.ncbi.nlm.nih.gov/pubmed/31752075
http://dx.doi.org/10.3390/molecules24224172
Descripción
Sumario:The fabrication of controlled supramolecular nanostructures via self-assembly of protoporphyrin IX (PPIX) was studied with enantiomerically pure l-arginine and d-arginine, and we have shown that stoichiometry controlled the morphology formed. The nanostructure morphology was mainly influenced by the delicate balance of π-π stacking interactions between PPIX cores, as well as H-bonding between the deprotonated acidic head group of PPIX with the guanidine head group of arginine. PPIX self-assembled with l-/d-arginine to create rose-like nanoflower structures for four equivalents of arginine that were 5–10 μm in length and 1–4 μm diameter. We employed UV-vis, fluorescence spectroscopy, scanning electron microscopy (SEM), X-ray diffraction (XRD), dynamic light scattering (DLS) and Fourier transform infrared spectroscopy (FT-IR) techniques to characterize the resulting self-assembled nanostructures. Furthermore, we investigated the catalytic activity of PPIX and arginine co-assembled materials. The fabricated PPIX–arginine nanostructure showed high enhancement of photocatalytic activity through degradation of rhodamine B (RhB) with a decrease in dye concentration of around 78–80% under simulated visible radiation.