Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics

Background and Objectives: All-ceramic prosthesis is widely used in modern dental practice because of its improved physico-mechanical and optical properties. These restorations are exposed to coloring agents from various nutrition and beverages in the oral cavity. Long-term color stability is critic...

Descripción completa

Detalles Bibliográficos
Autores principales: Haralur, Satheesh B., Raqe S. Alqahtani, Noura, Alhassan Mujayri, Fatimah
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6915526/
https://www.ncbi.nlm.nih.gov/pubmed/31752316
http://dx.doi.org/10.3390/medicina55110749
_version_ 1783480036828905472
author Haralur, Satheesh B.
Raqe S. Alqahtani, Noura
Alhassan Mujayri, Fatimah
author_facet Haralur, Satheesh B.
Raqe S. Alqahtani, Noura
Alhassan Mujayri, Fatimah
author_sort Haralur, Satheesh B.
collection PubMed
description Background and Objectives: All-ceramic prosthesis is widely used in modern dental practice because of its improved physico-mechanical and optical properties. These restorations are exposed to coloring agents from various nutrition and beverages in the oral cavity. Long-term color stability is critical for the success of these restorative materials. The purpose of this in vitro study was to assess the effect of common beverages and mouthwash on the color stability of lithium disilicate (LD), monolithic zirconia (MZ) and bilayer zirconia (BZ) surfaces. Materials and Method: Thirty disc-shaped specimens from each material were fabricated; each group was subdivided (n = 10) according to coffee, green tea and chlorhexidine immersion solutions. The baseline color of ceramic discs was recorded according to the CIE L*a*b* system with a portable spectrophotometer. The second measurement was recorded after 3000 thermocycling and immersion in coloring agents for 7 days. The mean color difference was calculated and data were compared with Kruskal-Wallis and Mann-Whitney post hoc tests (0.05). Results: ΔE values for LD with the immersion of coffee, tea, and Chlorhexidine gluconate (CHG) were 1.78, 2.241 and 1.58, respectively. Corresponding ΔE values for MZ were 5.60, 5.19, and 4.86; marginally higher than the clinically acceptable level of 3.5. Meanwhile, BZ showed better color stability compared to MZ with ΔE values of 4.22, 2.11 and 1.43. Conclusions: Among the ceramics evaluated, LD ceramic was found to be more color stable, while MZ ceramics displayed a higher susceptibility to discoloration. MZ and BZ ceramic colors were significantly altered with coffee immersion, while LD ceramics were more affected by green tea.
format Online
Article
Text
id pubmed-6915526
institution National Center for Biotechnology Information
language English
publishDate 2019
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-69155262019-12-24 Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics Haralur, Satheesh B. Raqe S. Alqahtani, Noura Alhassan Mujayri, Fatimah Medicina (Kaunas) Article Background and Objectives: All-ceramic prosthesis is widely used in modern dental practice because of its improved physico-mechanical and optical properties. These restorations are exposed to coloring agents from various nutrition and beverages in the oral cavity. Long-term color stability is critical for the success of these restorative materials. The purpose of this in vitro study was to assess the effect of common beverages and mouthwash on the color stability of lithium disilicate (LD), monolithic zirconia (MZ) and bilayer zirconia (BZ) surfaces. Materials and Method: Thirty disc-shaped specimens from each material were fabricated; each group was subdivided (n = 10) according to coffee, green tea and chlorhexidine immersion solutions. The baseline color of ceramic discs was recorded according to the CIE L*a*b* system with a portable spectrophotometer. The second measurement was recorded after 3000 thermocycling and immersion in coloring agents for 7 days. The mean color difference was calculated and data were compared with Kruskal-Wallis and Mann-Whitney post hoc tests (0.05). Results: ΔE values for LD with the immersion of coffee, tea, and Chlorhexidine gluconate (CHG) were 1.78, 2.241 and 1.58, respectively. Corresponding ΔE values for MZ were 5.60, 5.19, and 4.86; marginally higher than the clinically acceptable level of 3.5. Meanwhile, BZ showed better color stability compared to MZ with ΔE values of 4.22, 2.11 and 1.43. Conclusions: Among the ceramics evaluated, LD ceramic was found to be more color stable, while MZ ceramics displayed a higher susceptibility to discoloration. MZ and BZ ceramic colors were significantly altered with coffee immersion, while LD ceramics were more affected by green tea. MDPI 2019-11-19 /pmc/articles/PMC6915526/ /pubmed/31752316 http://dx.doi.org/10.3390/medicina55110749 Text en © 2019 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Haralur, Satheesh B.
Raqe S. Alqahtani, Noura
Alhassan Mujayri, Fatimah
Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
title Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
title_full Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
title_fullStr Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
title_full_unstemmed Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
title_short Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
title_sort effect of hydrothermal aging and beverages on color stability of lithium disilicate and zirconia based ceramics
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6915526/
https://www.ncbi.nlm.nih.gov/pubmed/31752316
http://dx.doi.org/10.3390/medicina55110749
work_keys_str_mv AT haralursatheeshb effectofhydrothermalagingandbeveragesoncolorstabilityoflithiumdisilicateandzirconiabasedceramics
AT raqesalqahtaninoura effectofhydrothermalagingandbeveragesoncolorstabilityoflithiumdisilicateandzirconiabasedceramics
AT alhassanmujayrifatimah effectofhydrothermalagingandbeveragesoncolorstabilityoflithiumdisilicateandzirconiabasedceramics