Cargando…

The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads

In this study, the effect of the ionic cross-linking mode on the ability to control physical properties and in vitro release behavior of the dexamethasone (DEX) drug from chitosan (CS) and chitosan/hydroxyapatite (CS/HA) beads was investigated. CS solutions without and with HA and DEX were dripped i...

Descripción completa

Detalles Bibliográficos
Autores principales: L. Dantas, Maria Jucélia, F. dos Santos, Bárbara Fernanda, A. Tavares, Albaniza, Maciel, Matheus A., Lucena, Breno de Medeiros, L. Fook, Marcus Vinícius, de L. Silva, Suédina Maria
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6943658/
https://www.ncbi.nlm.nih.gov/pubmed/31835480
http://dx.doi.org/10.3390/molecules24244510
_version_ 1783484926351376384
author L. Dantas, Maria Jucélia
F. dos Santos, Bárbara Fernanda
A. Tavares, Albaniza
Maciel, Matheus A.
Lucena, Breno de Medeiros
L. Fook, Marcus Vinícius
de L. Silva, Suédina Maria
author_facet L. Dantas, Maria Jucélia
F. dos Santos, Bárbara Fernanda
A. Tavares, Albaniza
Maciel, Matheus A.
Lucena, Breno de Medeiros
L. Fook, Marcus Vinícius
de L. Silva, Suédina Maria
author_sort L. Dantas, Maria Jucélia
collection PubMed
description In this study, the effect of the ionic cross-linking mode on the ability to control physical properties and in vitro release behavior of the dexamethasone (DEX) drug from chitosan (CS) and chitosan/hydroxyapatite (CS/HA) beads was investigated. CS solutions without and with HA and DEX were dripped into two coagulation solutions, prepared with a non-toxic ionic crosslinker (sodium tripolyphosphate, TPP) and distilled water, one at pH = 9.0 and other at pH = 6.0. Optical microscopy (OM) and scanning electron microscopy (SEM) results showed changes on the surface topology of the beads, with a reduction of roughness for beads prepared at pH = 6.0 and an increase for the one prepared at pH = 9.0. The diameter and sphericity of the beads prepared at pH = 6.0 proved more uniform and had a larger pore size with a good interconnectivity framework. Attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR) suggested a higher crosslinking degree for beads prepared at pH = 6.0, corroborated by X-ray diffraction profiles (XRD) analysis that indicated a decrease in the crystalline structure for such beads. In in vitro drug release data, all beads presented a sustained release during the studied period (24 h). The drug release rate was affected by the pH of the coagulation solution used in the preparation of the beads. The in vitro kinetics of the release process was of the Peppas–Sahlin model, controlled by both diffusion and relaxation of polymer chains or swelling (anomalous transport mechanism). Our results suggest that DEX-loaded CS/HA beads, crosslinked in TPP coagulation solution at pH = 9.0, led to a decrease in the DEX release rate and prolonged the release period. Thus, this composition might have prospective as a functional material for bone and cartilage tissue engineering.
format Online
Article
Text
id pubmed-6943658
institution National Center for Biotechnology Information
language English
publishDate 2019
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-69436582020-01-10 The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads L. Dantas, Maria Jucélia F. dos Santos, Bárbara Fernanda A. Tavares, Albaniza Maciel, Matheus A. Lucena, Breno de Medeiros L. Fook, Marcus Vinícius de L. Silva, Suédina Maria Molecules Article In this study, the effect of the ionic cross-linking mode on the ability to control physical properties and in vitro release behavior of the dexamethasone (DEX) drug from chitosan (CS) and chitosan/hydroxyapatite (CS/HA) beads was investigated. CS solutions without and with HA and DEX were dripped into two coagulation solutions, prepared with a non-toxic ionic crosslinker (sodium tripolyphosphate, TPP) and distilled water, one at pH = 9.0 and other at pH = 6.0. Optical microscopy (OM) and scanning electron microscopy (SEM) results showed changes on the surface topology of the beads, with a reduction of roughness for beads prepared at pH = 6.0 and an increase for the one prepared at pH = 9.0. The diameter and sphericity of the beads prepared at pH = 6.0 proved more uniform and had a larger pore size with a good interconnectivity framework. Attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR) suggested a higher crosslinking degree for beads prepared at pH = 6.0, corroborated by X-ray diffraction profiles (XRD) analysis that indicated a decrease in the crystalline structure for such beads. In in vitro drug release data, all beads presented a sustained release during the studied period (24 h). The drug release rate was affected by the pH of the coagulation solution used in the preparation of the beads. The in vitro kinetics of the release process was of the Peppas–Sahlin model, controlled by both diffusion and relaxation of polymer chains or swelling (anomalous transport mechanism). Our results suggest that DEX-loaded CS/HA beads, crosslinked in TPP coagulation solution at pH = 9.0, led to a decrease in the DEX release rate and prolonged the release period. Thus, this composition might have prospective as a functional material for bone and cartilage tissue engineering. MDPI 2019-12-10 /pmc/articles/PMC6943658/ /pubmed/31835480 http://dx.doi.org/10.3390/molecules24244510 Text en © 2019 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
L. Dantas, Maria Jucélia
F. dos Santos, Bárbara Fernanda
A. Tavares, Albaniza
Maciel, Matheus A.
Lucena, Breno de Medeiros
L. Fook, Marcus Vinícius
de L. Silva, Suédina Maria
The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads
title The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads
title_full The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads
title_fullStr The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads
title_full_unstemmed The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads
title_short The Impact of the Ionic Cross-Linking Mode on the Physical and In Vitro Dexamethasone Release Properties of Chitosan/Hydroxyapatite Beads
title_sort impact of the ionic cross-linking mode on the physical and in vitro dexamethasone release properties of chitosan/hydroxyapatite beads
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6943658/
https://www.ncbi.nlm.nih.gov/pubmed/31835480
http://dx.doi.org/10.3390/molecules24244510
work_keys_str_mv AT ldantasmariajucelia theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT fdossantosbarbarafernanda theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT atavaresalbaniza theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT macielmatheusa theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT lucenabrenodemedeiros theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT lfookmarcusvinicius theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT delsilvasuedinamaria theimpactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT ldantasmariajucelia impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT fdossantosbarbarafernanda impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT atavaresalbaniza impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT macielmatheusa impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT lucenabrenodemedeiros impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT lfookmarcusvinicius impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads
AT delsilvasuedinamaria impactoftheioniccrosslinkingmodeonthephysicalandinvitrodexamethasonereleasepropertiesofchitosanhydroxyapatitebeads