Analysis of Plastic Deformation Instabilities at Elevated Temperatures in Hot-Rolled Medium-Mn Steel

The study addressed the microstructure and mechanical properties of hot-rolled advanced high-strength medium manganese steel. Some of the curves that were obtained in static tensile tests at deformation temperatures of 20–200 °C showed the occurrence of the heterogeneous plastic deformation phenomen...

Descripción completa

Detalles Bibliográficos
Autores principales: Kozłowska, Aleksandra, Grzegorczyk, Barbara, Staszuk, Marcin, Nuckowski, Paweł M., Grajcar, Adam
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6947337/
https://www.ncbi.nlm.nih.gov/pubmed/31842476
http://dx.doi.org/10.3390/ma12244184
Descripción
Sumario:The study addressed the microstructure and mechanical properties of hot-rolled advanced high-strength medium manganese steel. Some of the curves that were obtained in static tensile tests at deformation temperatures of 20–200 °C showed the occurrence of the heterogeneous plastic deformation phenomenon, called the Portevin-Le Chatelier (PLC) effect. The deformation temperature significantly influenced a serration character. The correlations between the deformation temperature, serration range, microstructural features, and fracture behavior were investigated. The curves showed no Lüders elongation as a result of the thermomechanical processing applied. The serrated flow phenomenon was observed at 60 and 140 °C. The serration type was different and the most enhanced at 140 °C, where the PLC effect was present in both uniform and post-uniform elongation ranges. The disappearance of serrations at 200 °C was related to the increased diffusion intensity.