Influence of Milling Time on the Homogeneity and Magnetism of a Fe(70)Zr(30) Partially Amorphous Alloy: Distribution of Curie Temperatures

In this work, the mechanically alloyed Fe(70)Zr(30) (at. %) composition has been used to study the influence of milling time on its homogeneity and magnetic properties. The microstructure and Fe environment results show the formation of an almost fully amorphous alloy after 50 h of milling in a mixt...

Descripción completa

Detalles Bibliográficos
Autores principales: Manchón-Gordón, Alejandro F., Ipus, Jhon J., Blázquez, Javier S., Conde, Clara F., Conde, Alejandro
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7014023/
https://www.ncbi.nlm.nih.gov/pubmed/31968600
http://dx.doi.org/10.3390/ma13020490
Descripción
Sumario:In this work, the mechanically alloyed Fe(70)Zr(30) (at. %) composition has been used to study the influence of milling time on its homogeneity and magnetic properties. The microstructure and Fe environment results show the formation of an almost fully amorphous alloy after 50 h of milling in a mixture of pure 70 at. % Fe and 30 at. % Zr. The soft magnetic behavior of the samples enhances with the increase of the milling time, which is ascribed to the averaging out of the magnetocrystalline anisotropy as the crystal size decreases and the amorphous fraction increases. The formation of a non-perfectly homogenous system leads to a certain compositional heterogeneity, motivating the existence of a distribution of Curie temperatures. The parameters of the distribution (the average Curie temperature, [Formula: see text] , and the broadening of the distribution, [Formula: see text]) have been obtained using a recently reported procedure, based on the analysis of the approach towards the saturation curves and the magnetocaloric effect. The decrease of [Formula: see text] and the increase of [Formula: see text] with the milling time are in agreement with the microstructural results. As the remaining α-Fe phase decreases, the amorphous matrix is enriched in Fe atoms, enhancing its magnetic response.