In order to improve the interfacial bonding between hydroxyapatite (HAP) and poly-l-lactic acid (PLLA), 2-Carboxyethylphosphonic acid (CEPA), a phosphonic acid coupling agent, was introduced to modify HAP nanoparticles. After this. the PLLA scaffold containing CEPA-modified HAP (C-HAP) was fabricate...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7023562/ https://www.ncbi.nlm.nih.gov/pubmed/31940986 http://dx.doi.org/10.3390/polym12010199 |
Sumario: | In order to improve the interfacial bonding between hydroxyapatite (HAP) and poly-l-lactic acid (PLLA), 2-Carboxyethylphosphonic acid (CEPA), a phosphonic acid coupling agent, was introduced to modify HAP nanoparticles. After this. the PLLA scaffold containing CEPA-modified HAP (C-HAP) was fabricated by selective laser sintering (frittage). The specific mechanism of interfacial bonding was that the PO(3)(2−) of CEPA formed an electrovalent bond with the Ca(2+) of HAP on one hand, and on the other hand, the –COOH of CEPA formed an ester bond with the –OH of PLLA via an esterification reaction. The results showed that C-HAP was homogeneously dispersed in the PLLA matrix and that it exhibited interconnected morphology pulled out from the PLLA matrix due to the enhanced interfacial bonding. As a result, the tensile strength and modulus of the scaffold with 20% C-HAP increased by 1.40 and 2.79 times compared to that of the scaffold with HAP, respectively. In addition, the scaffold could attract Ca(2+) in simulated body fluid (SBF) solution by the phosphonic acid group to induce apatite layer formation and also release Ca(2+) and PO(4)(3−) by degradation to facilitate cell attachment, growth and proliferation. |
---|