Cargando…

Preparation of Black Ceramic Tiles Using Waste Copper Slag and Stainless Steel Slag of Electric Arc Furnace

Copper slag and stainless steel slag of Electric Arc Furnace (EAF) are two typical metallurgical solid wastes, which contain a large number of valuables, such as Fe, Cr, and Cu. The transition metal elements in the waste slags, such as Cr and Fe, can be recycled as the coloring ions in the black cer...

Descripción completa

Detalles Bibliográficos
Autores principales: Liu, Mengke, Ma, Guojun, Zhang, Xiang, Liu, Junjie, Wang, Qiang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7040580/
https://www.ncbi.nlm.nih.gov/pubmed/32046250
http://dx.doi.org/10.3390/ma13030776
Descripción
Sumario:Copper slag and stainless steel slag of Electric Arc Furnace (EAF) are two typical metallurgical solid wastes, which contain a large number of valuables, such as Fe, Cr, and Cu. The transition metal elements in the waste slags, such as Cr and Fe, can be recycled as the coloring ions in the black ceramic tile. In this study, the Fe/Cr molar ratio in the raw materials of copper slag and stainless steel slag was adjusted, and the black ceramic tile was subsequently prepared by sintering. The results show that the optimum process parameters for the preparation of black ceramic tiles are the Fe/Cr molar ratio of 2.0, the sintering temperature of 1150 °C, and the sintering time of 30 min. The compressive strength of the black ceramic tile at optimum sintering conditions exceeds the minimum compressive strength of the Chinese national standard for standard polished tiles, and the concentrations of harmful elements, for example, Cr, Cu, Ni, As, Zn, Pb, and Cr(VI) are within the regulation thresholds specified by the Chinese national standard.