Cargando…

Correlation between phase compatibility and efficient energy conversion in Zr-doped Barium Titanate

Recent demonstrations of both heat-to-electricity energy conversion devices and electrocaloric devices based on first-order ferroelectric phase transformations identify the lowering of hysteresis and cyclic reversibility of the transformation as enabling criteria for the advancement of this technolo...

Descripción completa

Detalles Bibliográficos
Autores principales: Wegner, Maike, Gu, Hanlin, James, Richard D., Quandt, Eckhard
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7044276/
https://www.ncbi.nlm.nih.gov/pubmed/32103069
http://dx.doi.org/10.1038/s41598-020-60335-5
Descripción
Sumario:Recent demonstrations of both heat-to-electricity energy conversion devices and electrocaloric devices based on first-order ferroelectric phase transformations identify the lowering of hysteresis and cyclic reversibility of the transformation as enabling criteria for the advancement of this technology. These demonstrations, and recent studies of the hysteresis of phase transformations in oxides, show that satisfying conditions of supercompatibility can be useful for lowering hysteresis, but with limitations for systems with only a few variants of the lower symmetry phase. In particular, it is widely accepted that in a classic cubic-to-tetragonal phase transformation, with only three tetragonal variants having only six twin systems, tuning for improved crystallographic compatibility will be of limited value. This work shows that, on the contrary, the tuning of lattice parameters in Ba(Ti(1-x)Zr(x))O(3) for improved crystallographic compatibility, even at low doping levels of Zr (x ≤ 0.027), give significant improvement of transformation and ferroelectric energy conversion properties. Specifically, the transformation hysteresis is lowered by 25%, and the maximum value of the polarization/temperature ratio dP/dT at the phase transformation is increased by 10%.