Cargando…
ATR-FTIR Analysis and One-Week Stress Relaxation of Four Orthodontic Aligner Materials
The aim of this study was to estimate possible differences in the chemical composition and relaxation of orthodontic aligner materials. Four commercially available thermoplastic materials CAM (Scheu-Dental, Iserlohn, Germany), COP (Essix, Dentsply Raintree Essix Sarasota, FL, USA), DUR (Great Lakes...
Autores principales: | Jaggy, Florina, Zinelis, Spiros, Polychronis, Georgios, Patcas, Raphael, Schätzle, Marc, Eliades, George, Eliades, Theodore |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7215293/ https://www.ncbi.nlm.nih.gov/pubmed/32316154 http://dx.doi.org/10.3390/ma13081868 |
Ejemplares similares
-
Εffect of cleansers on the composition and mechanical properties of orthodontic aligners in vitro
por: Iliadi, Anna, et al.
Publicado: (2022) -
Comparative analysis of mechanical properties of orthodontic aligners produced by different contemporary 3D printers
por: Zinelis, Spiros, et al.
Publicado: (2021) -
Changes in Roughness and Mechanical Properties of Invisalign(®) Appliances after One- and Two-Weeks Use
por: Papadopoulou, Alexandra K., et al.
Publicado: (2019) -
Mechanical properties of orthodontic wires derived by instrumented indentation testing (IIT) according to ISO 14577
por: Zinelis, Spiros, et al.
Publicado: (2015) -
Orthodontic bonding and debonding induces structural changes but does not alter the mechanical properties of enamel
por: Ioannidis, Alexis, et al.
Publicado: (2018)