The Influence of Powder Milling on Properties of SPS Compacted FeAl
The Fe-28 at.% Al alloy was studied in this article. The aim was to describe the influence of gas atomized powder pre-milling before SPS (Spark Plasma Sintering) sintering on the structure and properties of the bulk materials. The initial powder was milled for 0.5, 1, and 8 h. It was proven that 1 h...
Autores principales: | , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7248823/ https://www.ncbi.nlm.nih.gov/pubmed/32403351 http://dx.doi.org/10.3390/molecules25092263 |
_version_ | 1783538460034859008 |
---|---|
author | Michalcová, Alena Özkan, Murat Mikula, Pavol Marek, Ivo Knaislová, Anna Kopeček, Jaromír Vojtěch, Dalibor |
author_facet | Michalcová, Alena Özkan, Murat Mikula, Pavol Marek, Ivo Knaislová, Anna Kopeček, Jaromír Vojtěch, Dalibor |
author_sort | Michalcová, Alena |
collection | PubMed |
description | The Fe-28 at.% Al alloy was studied in this article. The aim was to describe the influence of gas atomized powder pre-milling before SPS (Spark Plasma Sintering) sintering on the structure and properties of the bulk materials. The initial powder was milled for 0.5, 1, and 8 h. It was proven that 1 h milling leads to the change in size and morphology of the particles, B2→A2 phase transformation, and to the contamination with the material from a milling vessel. Powder materials were compacted by the SPS process at 900, 1000, and 1100 °C. The differences between the bulk materials were tested by LM, SEM, and TEM microscopy, XRD, and neutron diffraction methods. It was proven that, although the structures of initial powder (B2) and milled powder (A2) were different, both provide after-sintering material with the same structure (D0(3)) with similar structural parameters. Higher hardness and improved ductility of the material sintered from the milled powder are likely caused by the change in chemical composition during the milling process. |
format | Online Article Text |
id | pubmed-7248823 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2020 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-72488232020-06-10 The Influence of Powder Milling on Properties of SPS Compacted FeAl Michalcová, Alena Özkan, Murat Mikula, Pavol Marek, Ivo Knaislová, Anna Kopeček, Jaromír Vojtěch, Dalibor Molecules Article The Fe-28 at.% Al alloy was studied in this article. The aim was to describe the influence of gas atomized powder pre-milling before SPS (Spark Plasma Sintering) sintering on the structure and properties of the bulk materials. The initial powder was milled for 0.5, 1, and 8 h. It was proven that 1 h milling leads to the change in size and morphology of the particles, B2→A2 phase transformation, and to the contamination with the material from a milling vessel. Powder materials were compacted by the SPS process at 900, 1000, and 1100 °C. The differences between the bulk materials were tested by LM, SEM, and TEM microscopy, XRD, and neutron diffraction methods. It was proven that, although the structures of initial powder (B2) and milled powder (A2) were different, both provide after-sintering material with the same structure (D0(3)) with similar structural parameters. Higher hardness and improved ductility of the material sintered from the milled powder are likely caused by the change in chemical composition during the milling process. MDPI 2020-05-11 /pmc/articles/PMC7248823/ /pubmed/32403351 http://dx.doi.org/10.3390/molecules25092263 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Michalcová, Alena Özkan, Murat Mikula, Pavol Marek, Ivo Knaislová, Anna Kopeček, Jaromír Vojtěch, Dalibor The Influence of Powder Milling on Properties of SPS Compacted FeAl |
title | The Influence of Powder Milling on Properties of SPS Compacted FeAl |
title_full | The Influence of Powder Milling on Properties of SPS Compacted FeAl |
title_fullStr | The Influence of Powder Milling on Properties of SPS Compacted FeAl |
title_full_unstemmed | The Influence of Powder Milling on Properties of SPS Compacted FeAl |
title_short | The Influence of Powder Milling on Properties of SPS Compacted FeAl |
title_sort | influence of powder milling on properties of sps compacted feal |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7248823/ https://www.ncbi.nlm.nih.gov/pubmed/32403351 http://dx.doi.org/10.3390/molecules25092263 |
work_keys_str_mv | AT michalcovaalena theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT ozkanmurat theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT mikulapavol theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT marekivo theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT knaislovaanna theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT kopecekjaromir theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT vojtechdalibor theinfluenceofpowdermillingonpropertiesofspscompactedfeal AT michalcovaalena influenceofpowdermillingonpropertiesofspscompactedfeal AT ozkanmurat influenceofpowdermillingonpropertiesofspscompactedfeal AT mikulapavol influenceofpowdermillingonpropertiesofspscompactedfeal AT marekivo influenceofpowdermillingonpropertiesofspscompactedfeal AT knaislovaanna influenceofpowdermillingonpropertiesofspscompactedfeal AT kopecekjaromir influenceofpowdermillingonpropertiesofspscompactedfeal AT vojtechdalibor influenceofpowdermillingonpropertiesofspscompactedfeal |