Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns

Objectives  The aim of this study was to compare the effects of two margin designs (shoulderless and slight chamfer) with two occlusal thicknesses on fracture resistance and failure mode of the monolithic zirconia crowns. Materials and Methods  Forty nickel–chromium dies were duplicated from the pre...

Descripción completa

Detalles Bibliográficos
Autores principales: Jasim, Haider Hasan, Findakly, Meelad Basil, Mahdi, Nada Ali, Mutar, Mustafa Tariq
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Thieme Medical and Scientific Publishers Private Ltd. 2020
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7274823/
https://www.ncbi.nlm.nih.gov/pubmed/32503065
http://dx.doi.org/10.1055/s-0040-1709342
_version_ 1783542668678135808
author Jasim, Haider Hasan
Findakly, Meelad Basil
Mahdi, Nada Ali
Mutar, Mustafa Tariq
author_facet Jasim, Haider Hasan
Findakly, Meelad Basil
Mahdi, Nada Ali
Mutar, Mustafa Tariq
author_sort Jasim, Haider Hasan
collection PubMed
description Objectives  The aim of this study was to compare the effects of two margin designs (shoulderless and slight chamfer) with two occlusal thicknesses on fracture resistance and failure mode of the monolithic zirconia crowns. Materials and Methods  Forty nickel–chromium dies were duplicated from the previous two prepared teeth using a three-dimensional optical scanner. Nickel–chromium supporting dies were divided into two main groups ( n = 20) according to the type of margin design: group A, slight chamfer margin design and group B, shoulderless margin design. These groups were further divided into two subgroups according to the occlusal thicknesses (0.5 and 1 mm). The digital imaging of each die was done using a three-dimensional optical scanner, then zirconia blocks were milled by 5-axis machine. The crowns were cleaned by alcohol, air dried, and cemented by resin cement. Next, the crowns were subjected to 500 hot and cold cycles (30 seconds for each cycle). The samples were subjected to a static load until failure using an electronic universal testing machine and fracture resistance was recorded in Newton (N). Statistical Analysis  Data were analyzed using the test of normality (Shapiro–Wilk test) and two-way analysis of variance (ANOVA) test. Results   The highest mean fracture load was recorded by the shoulderless (1 mm occlusal thickness) subgroup (3,992.5 N), followed by shoulderless (0.5 mm occlusal thickness) subgroup (3,244.4 N), and the slight chamfer (1 mm occlusal thickness) subgroup (2,811 N). The lowest mean of fracture load was recorded by slight chamfer (0.5 mm occlusal thickness) subgroup (1,632.9 N). The two-way ANOVA test revealed a significant difference between the four subgroups. Regarding the fracture mode, the slight chamfer subgroups showed a severe fracture of the restoration while the shoulderless subgroups showed a fracture through the midline of the restoration. Conclusion  Within the limitation of the comparative study, shoulderless margin design has a more favorable outcome than a slight chamfer design in all thicknesses. Although the restoration with reduced occlusal thickness has lower fracture resistance than 1 mm occlusal thickness, the 0.5 mm restorations still can tolerate occlusal forces.
format Online
Article
Text
id pubmed-7274823
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher Thieme Medical and Scientific Publishers Private Ltd.
record_format MEDLINE/PubMed
spelling pubmed-72748232020-06-10 Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns Jasim, Haider Hasan Findakly, Meelad Basil Mahdi, Nada Ali Mutar, Mustafa Tariq Eur J Dent Objectives  The aim of this study was to compare the effects of two margin designs (shoulderless and slight chamfer) with two occlusal thicknesses on fracture resistance and failure mode of the monolithic zirconia crowns. Materials and Methods  Forty nickel–chromium dies were duplicated from the previous two prepared teeth using a three-dimensional optical scanner. Nickel–chromium supporting dies were divided into two main groups ( n = 20) according to the type of margin design: group A, slight chamfer margin design and group B, shoulderless margin design. These groups were further divided into two subgroups according to the occlusal thicknesses (0.5 and 1 mm). The digital imaging of each die was done using a three-dimensional optical scanner, then zirconia blocks were milled by 5-axis machine. The crowns were cleaned by alcohol, air dried, and cemented by resin cement. Next, the crowns were subjected to 500 hot and cold cycles (30 seconds for each cycle). The samples were subjected to a static load until failure using an electronic universal testing machine and fracture resistance was recorded in Newton (N). Statistical Analysis  Data were analyzed using the test of normality (Shapiro–Wilk test) and two-way analysis of variance (ANOVA) test. Results   The highest mean fracture load was recorded by the shoulderless (1 mm occlusal thickness) subgroup (3,992.5 N), followed by shoulderless (0.5 mm occlusal thickness) subgroup (3,244.4 N), and the slight chamfer (1 mm occlusal thickness) subgroup (2,811 N). The lowest mean of fracture load was recorded by slight chamfer (0.5 mm occlusal thickness) subgroup (1,632.9 N). The two-way ANOVA test revealed a significant difference between the four subgroups. Regarding the fracture mode, the slight chamfer subgroups showed a severe fracture of the restoration while the shoulderless subgroups showed a fracture through the midline of the restoration. Conclusion  Within the limitation of the comparative study, shoulderless margin design has a more favorable outcome than a slight chamfer design in all thicknesses. Although the restoration with reduced occlusal thickness has lower fracture resistance than 1 mm occlusal thickness, the 0.5 mm restorations still can tolerate occlusal forces. Thieme Medical and Scientific Publishers Private Ltd. 2020-05 2020-06-05 /pmc/articles/PMC7274823/ /pubmed/32503065 http://dx.doi.org/10.1055/s-0040-1709342 Text en https://creativecommons.org/licenses/by-nc-nd/4.0/ This is an open-access article distributed under the terms of the Creative Commons Attribution-NonCommercial-NoDerivatives License, which permits unrestricted reproduction and distribution, for non-commercial purposes only; and use and reproduction, but not distribution, of adapted material for non-commercial purposes only, provided the original work is properly cited.
spellingShingle Jasim, Haider Hasan
Findakly, Meelad Basil
Mahdi, Nada Ali
Mutar, Mustafa Tariq
Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns
title Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns
title_full Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns
title_fullStr Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns
title_full_unstemmed Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns
title_short Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns
title_sort effect of reduced occlusal thickness with two margin designs on fracture resistance of monolithic zirconia crowns
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7274823/
https://www.ncbi.nlm.nih.gov/pubmed/32503065
http://dx.doi.org/10.1055/s-0040-1709342
work_keys_str_mv AT jasimhaiderhasan effectofreducedocclusalthicknesswithtwomargindesignsonfractureresistanceofmonolithiczirconiacrowns
AT findaklymeeladbasil effectofreducedocclusalthicknesswithtwomargindesignsonfractureresistanceofmonolithiczirconiacrowns
AT mahdinadaali effectofreducedocclusalthicknesswithtwomargindesignsonfractureresistanceofmonolithiczirconiacrowns
AT mutarmustafatariq effectofreducedocclusalthicknesswithtwomargindesignsonfractureresistanceofmonolithiczirconiacrowns