Ultrastable Sodium–Sulfur Batteries without Polysulfides Formation Using Slit Ultramicropore Carbon Carrier
The formation of the soluble polysulfides (Na(2)S(n), 4 ≤ n ≤ 8) causes poor cycling performance for room temperature sodium–sulfur (RT Na–S) batteries. Moreover, the formation of insoluble polysulfides (Na(2)S(n), 2 ≤ n < 4) can slow down the reaction kinetics and terminate the discharge reactio...
Autores principales: | Guo, Qiubo, Li, Shuang, Liu, Xuejun, Lu, Haochen, Chang, Xiaoqing, Zhang, Hongshen, Zhu, Xiaohui, Xia, Qiuying, Yan, Chenglin, Xia, Hui |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
John Wiley and Sons Inc.
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7284216/ https://www.ncbi.nlm.nih.gov/pubmed/32537400 http://dx.doi.org/10.1002/advs.201903246 |
Ejemplares similares
-
Insight into Sulfur Confined in Ultramicroporous Carbon
por: Helen, M., et al.
Publicado: (2018) -
Polysulfide Catalytic Materials for Fast‐Kinetic Metal–Sulfur Batteries: Principles and Active Centers
por: Cheng, Menghao, et al.
Publicado: (2021) -
Confined Polysulfides in N-Doped 3D-CNTs Network for High Performance Lithium-Sulfur Batteries
por: Wang, Donghuang, et al.
Publicado: (2021) -
Chemisorption of polysulfides through redox reactions with organic molecules for lithium–sulfur batteries
por: Li, Ge, et al.
Publicado: (2018) -
Attention-based solubility prediction of polysulfide and electrolyte analysis for lithium–sulfur batteries
por: Lee, Jaewan, et al.
Publicado: (2023)