Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications

Tetracalcium phosphate (TTCP), a potential biological scaffold material, has attracted increasing interest for bone regeneration applications due to its good biodegradability and biocompatibility. In this research, three-dimensional porous TTCP scaffolds were manufactured via selective laser sinteri...

Descripción completa

Detalles Bibliográficos
Autores principales: Qin, Tian, Li, Xiaoqian, Long, Hui, Bin, Shizhen, Xu, Yong
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7287688/
https://www.ncbi.nlm.nih.gov/pubmed/32423078
http://dx.doi.org/10.3390/ma13102268
_version_ 1783545106295422976
author Qin, Tian
Li, Xiaoqian
Long, Hui
Bin, Shizhen
Xu, Yong
author_facet Qin, Tian
Li, Xiaoqian
Long, Hui
Bin, Shizhen
Xu, Yong
author_sort Qin, Tian
collection PubMed
description Tetracalcium phosphate (TTCP), a potential biological scaffold material, has attracted increasing interest for bone regeneration applications due to its good biodegradability and biocompatibility. In this research, three-dimensional porous TTCP scaffolds were manufactured via selective laser sintering (SLS), and an in-depth and meticulous study on the influence of laser power on the microstructure and mechanical properties of TTCP scaffolds was performed. The results showed that the TTCP particles fused together and formed a solid object due to the decrease in the number of micro-pores in the scaffold as the laser power increased from 6 W to 9 W. The maximum compressive strength that the scaffold could withstand and the strength of the fracture toughness were 11.87 ± 0.64 MPa and 1.12 ± 0.1 MPa·m(1/2), respectively. When the laser power increased from 9 W to 10 W, the TTCP grains grew abnormally, resulting in diminished mechanical properties. The bioactivity tests showed that the surfaces of the scaffolds were entirely covered by bone-like apatite layers after soaking in simulated body fluid (SBF) for three days, indicating that the scaffolds exhibit excellent bioactivity. Moreover, cell experiments showed that the TTCP scaffolds had good biocompatibility. This study indicated that SLS-fabricated TTCP scaffolds may be a promising candidate for bone regeneration applications.
format Online
Article
Text
id pubmed-7287688
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-72876882020-06-15 Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications Qin, Tian Li, Xiaoqian Long, Hui Bin, Shizhen Xu, Yong Materials (Basel) Article Tetracalcium phosphate (TTCP), a potential biological scaffold material, has attracted increasing interest for bone regeneration applications due to its good biodegradability and biocompatibility. In this research, three-dimensional porous TTCP scaffolds were manufactured via selective laser sintering (SLS), and an in-depth and meticulous study on the influence of laser power on the microstructure and mechanical properties of TTCP scaffolds was performed. The results showed that the TTCP particles fused together and formed a solid object due to the decrease in the number of micro-pores in the scaffold as the laser power increased from 6 W to 9 W. The maximum compressive strength that the scaffold could withstand and the strength of the fracture toughness were 11.87 ± 0.64 MPa and 1.12 ± 0.1 MPa·m(1/2), respectively. When the laser power increased from 9 W to 10 W, the TTCP grains grew abnormally, resulting in diminished mechanical properties. The bioactivity tests showed that the surfaces of the scaffolds were entirely covered by bone-like apatite layers after soaking in simulated body fluid (SBF) for three days, indicating that the scaffolds exhibit excellent bioactivity. Moreover, cell experiments showed that the TTCP scaffolds had good biocompatibility. This study indicated that SLS-fabricated TTCP scaffolds may be a promising candidate for bone regeneration applications. MDPI 2020-05-14 /pmc/articles/PMC7287688/ /pubmed/32423078 http://dx.doi.org/10.3390/ma13102268 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Qin, Tian
Li, Xiaoqian
Long, Hui
Bin, Shizhen
Xu, Yong
Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications
title Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications
title_full Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications
title_fullStr Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications
title_full_unstemmed Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications
title_short Bioactive Tetracalcium Phosphate Scaffolds Fabricated by Selective Laser Sintering for Bone Regeneration Applications
title_sort bioactive tetracalcium phosphate scaffolds fabricated by selective laser sintering for bone regeneration applications
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7287688/
https://www.ncbi.nlm.nih.gov/pubmed/32423078
http://dx.doi.org/10.3390/ma13102268
work_keys_str_mv AT qintian bioactivetetracalciumphosphatescaffoldsfabricatedbyselectivelasersinteringforboneregenerationapplications
AT lixiaoqian bioactivetetracalciumphosphatescaffoldsfabricatedbyselectivelasersinteringforboneregenerationapplications
AT longhui bioactivetetracalciumphosphatescaffoldsfabricatedbyselectivelasersinteringforboneregenerationapplications
AT binshizhen bioactivetetracalciumphosphatescaffoldsfabricatedbyselectivelasersinteringforboneregenerationapplications
AT xuyong bioactivetetracalciumphosphatescaffoldsfabricatedbyselectivelasersinteringforboneregenerationapplications