Characterization of the Uniformity of High-Flux CdZnTe Material

Since the late 2000s, the availability of high-quality cadmium zinc telluride (CdZnTe) has greatly increased. The excellent spectroscopic performance of this material has enabled the development of detectors with volumes exceeding 1 cm(3) for use in the detection of nuclear materials. CdZnTe is also...

Descripción completa

Detalles Bibliográficos
Autores principales: Veale, Matthew Charles, Booker, Paul, Cross, Simon, Hart, Matthew David, Jowitt, Lydia, Lipp, John, Schneider, Andreas, Seller, Paul, Wheater, Rhian Mair, Wilson, Matthew David, Hansson, Conny Christoffer Tobias, Iniewski, Krzysztof, Marthandam, Pramodha, Prekas, Georgios
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7294436/
https://www.ncbi.nlm.nih.gov/pubmed/32408497
http://dx.doi.org/10.3390/s20102747
Descripción
Sumario:Since the late 2000s, the availability of high-quality cadmium zinc telluride (CdZnTe) has greatly increased. The excellent spectroscopic performance of this material has enabled the development of detectors with volumes exceeding 1 cm(3) for use in the detection of nuclear materials. CdZnTe is also of great interest to the photon science community for applications in X-ray imaging cameras at synchrotron light sources and free electron lasers. Historically, spatial variations in the crystal properties and temporal instabilities under high-intensity irradiation has limited the use of CdZnTe detectors in these applications. Recently, Redlen Technologies have developed high-flux-capable CdZnTe material (HF-CdZnTe), which promises improved spatial and temporal stability. In this paper, the results of the characterization of 10 HF-CdZnTe detectors with dimensions of 20.35 mm × 20.45 mm × 2.00 mm are presented. Each sensor has 80 × 80 pixels on a 250-μm pitch and were flip-chip-bonded to the STFC HEXITEC ASIC. These devices show excellent spectroscopic performance at room temperature, with an average Full Width at Half Maximum (FWHM) of 0.83 keV measured at 59.54 keV. The effect of tellurium inclusions in these devices was found to be negligible; however, some detectors did show significant concentrations of scratches and dislocation walls. An investigation of the detector stability over 12 h of continuous operation showed negligible changes in performance.