Cargando…

Selective Adsorption and Electrocatalysis of Polysulfides through Hexatomic Nickel Clusters Embedded in N-Doped Graphene toward High-Performance Li-S Batteries

The shuttle effect hinders the practical application of lithium-sulfur (Li-S) batteries due to the poor affinity between a substrate and Li polysulfides (LiPSs) and the sluggish transition of soluble LiPSs to insoluble Li(2)S or elemental S. Here, we report that Ni hexatomic clusters embedded in a n...

Descripción completa

Detalles Bibliográficos
Autores principales: Ji, Jiapeng, Sha, Ying, Li, Zeheng, Gao, Xuehui, Zhang, Teng, Zhou, Shiyu, Qiu, Tong, Zhou, Shaodong, Zhang, Liang, Ling, Min, Hou, Yanglong, Liang, Chengdu
Formato: Online Artículo Texto
Lenguaje:English
Publicado: AAAS 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7335422/
https://www.ncbi.nlm.nih.gov/pubmed/32676587
http://dx.doi.org/10.34133/2020/5714349
Descripción
Sumario:The shuttle effect hinders the practical application of lithium-sulfur (Li-S) batteries due to the poor affinity between a substrate and Li polysulfides (LiPSs) and the sluggish transition of soluble LiPSs to insoluble Li(2)S or elemental S. Here, we report that Ni hexatomic clusters embedded in a nitrogen-doped three-dimensional (3D) graphene framework (Ni-N/G) possess stronger interaction with soluble polysulfides than that with insoluble polysulfides. The synthetic electrocatalyst deployed in the sulfur cathode plays a multifunctional role: (i) selectively adsorbing the polysulfides dissolved in the electrolyte, (ii) expediting the sluggish liquid-solid phase transformations at the active sites as electrocatalysts, and (iii) accelerating the kinetics of the electrochemical reaction of multielectron sulfur, thereby inhibiting the dissolution of LiPSs. The constructed S@Ni-N/G cathode delivers an areal capacity of 9.43 mAh cm(−2) at 0.1 C at S loading of 6.8 mg cm(−2), and it exhibits a gravimetric capacity of 1104 mAh g(−1) with a capacity fading rate of 0.045% per cycle over 50 cycles at 0.2 C at S loading of 2.0 mg cm(−2). This work opens a rational approach to achieve the selective adsorption and expediting of polysulfide transition for the performance enhancement of Li-S batteries.