To ascertain the influence of SiC nanowires on sintering kinetics of heterophase ceramics, two composite powders (TaSi(2)-TaC-SiC and TaSi(2)-TaC-SiC-SiC(nanowire)) are fabricated by mechanically activated combustion synthesis of Ta-Si-C and Ta-Si-C-(C(2)F(4)) reactive mixtures. Remarkable compressi...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7436015/ https://www.ncbi.nlm.nih.gov/pubmed/32751932 http://dx.doi.org/10.3390/ma13153394 |
Sumario: | To ascertain the influence of SiC nanowires on sintering kinetics of heterophase ceramics, two composite powders (TaSi(2)-TaC-SiC and TaSi(2)-TaC-SiC-SiC(nanowire)) are fabricated by mechanically activated combustion synthesis of Ta-Si-C and Ta-Si-C-(C(2)F(4)) reactive mixtures. Remarkable compressibility is achieved for the TaSi(2)-TaC-SiC-SiC(nanowire) composition (green density up to 84% as compared with 45.2% achieved for TaSi(2)-SiC-TaC) which is attributed to the lubricating effect of residual adsorbed fluorinated carbon (most likely C(4)F(8)). The outcomes of pressureless sintering of TaSi(2)-TaC-SiC and TaSi(2)-TaC-SiC-SiC(nanowire) compositions are vastly different; the former experiences no significant densification or grain growth and does not attain structural integrity, whereas the latter achieves relative density up to 93% and hardness up to 11 GPa. The SiC nanowires are not retained in consolidated ceramics, but instead, act as a sintering aid and promote densification and grain growth. Sintering mechanisms of TaSi(2)-TaC-SiC and TaSi(2)-TaC-SiC-SiC(nanowire) powders are analyzed using thermodynamic and ab initio grand potential calculations, as well as the analysis of grain size versus relative density relations. In the case of solid-state sintering, the densification and grain growth in heterophase non-oxide ceramics are governed by the same mechanisms as previously investigated single-phase oxides. The presence of SiC nanowires enhances grain-boundary related diffusion processes due to the high specific surface and aspect ratio of the nanowires. At 1500 °C, where the formation of the transient Si-based liquid phase is thermodynamically viable, only the SiC nanowire-containing composition demonstrated the intense grain coarsening and densification associated with liquid-assisted sintering. This effect can be attributed both to the presence of SiC nanowires and purification of residual oxide impurities due to C(2)F(4)-activated combustion synthesis employed for the in situ formation of SiC nanowires. |
---|