Synergistic Effect of the Total Acid Number, S, Cl, and H(2)O on the Corrosion of AISI 1020 in Acidic Environments
[Image: see text] The corrosive environment in sulfur-containing equipment is often complicated and changeable. This study adopted the Taguchi method to optimize the immersion test, and the L(27)(3(13)) orthogonal table was used to design an immersion corrosion experiment. The influence of four fact...
Autores principales: | Shen, Shuoxun, Wang, Zhirong, Jiang, Juncheng, Cao, Xingyan, Sun, Peipei, Lu, Yawei, Yang, Rongrong |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
American Chemical Society
2020
|
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7439373/ https://www.ncbi.nlm.nih.gov/pubmed/32832784 http://dx.doi.org/10.1021/acsomega.0c02219 |
Ejemplares similares
-
Statistical and Graphical Assessment of Circumferential and Radial Hardness Variation of AISI 4140, AISI 1020 and AA 6082 Aluminum Alloy
por: Al-Khalid, Hamad, et al.
Publicado: (2011) -
Proanthocyanidins with Corrosion Inhibition Activity
for AISI 1020 Carbon Steel under Neutral pH Conditions of Coconut
(Cocos nucifera L.) Husk Fibers
por: Guedes, Douglas, et al.
Publicado: (2021) -
Corrosion Behavior of Sensitized AISI 304 Stainless Steel in Acid Chloride Solution
por: Zatkalíková, Viera, et al.
Publicado: (2022) -
Fatigue Properties of Hot-Dip Galvanized AISI 1020 Normalized Steel in Tension–Compression and Tension–Tension Loading
por: Alweendo, Shatumbu Thomas, et al.
Publicado: (2021) -
Effects of elevated temperature on the corrosion resistance of silver–cobalt oxide–titanium dioxide (Ag/Co(3)O(4)/TiO(2)) nanocomposites coating on AISI 1020
por: Ibrahim, Mohammed, et al.
Publicado: (2021)